FRACTURE-MECHANICS OF TI/AL2O3 INTERFACES

被引:21
|
作者
WANG, HF [1 ]
GERBERICH, WW [1 ]
SKOWRONEK, CJ [1 ]
机构
[1] THREE M CO, MET MATRIX COMPOSITES PROGRAM, ST PAUL, MN 55144 USA
来源
ACTA METALLURGICA ET MATERIALIA | 1993年 / 41卷 / 08期
关键词
D O I
10.1016/0956-7151(93)90322-J
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Measurement of mixed mode interfacial fracture toughness in Ti/Al2O3 bimaterial couples has been accomplished by four-point bending tests of sandwich specimens with symmetrical cracks for different processing temperatures and thicknesses of Ti interlayers. Fracture surfaces and sample cross sections were analyzed by SEM, XPS, EDAX, EPMA and AES. The interfacial fracture toughness measured with four-point bending tests increases with increasing applied bonding temperature up to 950-degrees-C. Above this temperature toughness decreases. The deterioration of toughness is found to be due to an intermetallic phase (Ti3Al) produced by diffusion at high temperature. The interfacial fracture toughness also increases when the Ti interlayer is thicker. The measured critical strain energy release rate (or interfacial fracture energy) ranges from 10 to 45 J/m2. This is much larger than the estimated true work of adhesion which is about 2J/m2. This is because of plastic energy dissipation in the Ti interlayer during the fracture process.
引用
收藏
页码:2425 / 2432
页数:8
相关论文
共 50 条
  • [41] Interfaces in heterostructures of AlInGaN/GaN/Al2O3
    Zhou, Shengqiang
    Wu, M. F.
    Yao, S. D.
    Liu, J. P.
    Yang, H.
    SUPERLATTICES AND MICROSTRUCTURES, 2006, 39 (05) : 429 - 435
  • [42] Nitrogen passivation at GaAs:Al2O3 interfaces
    Guo, Yuzheng
    Lin, Liang
    Robertson, John
    APPLIED PHYSICS LETTERS, 2013, 102 (09)
  • [43] Interfaces Between CdTe and ALD Al2O3
    Perkins, Craig L.
    Ablekim, Tursun
    Barnes, Teresa M.
    Kuciauskas, Darius
    Lynn, Kelvin G.
    Nemeth, William
    Reese, Matthew O.
    Swain, Santosh K.
    Metzger, Wyatt K.
    IEEE JOURNAL OF PHOTOVOLTAICS, 2018, 8 (06): : 1858 - 1861
  • [44] Role of Ti diffusion on the formation of phases in the Al2O3–Al2O3 brazed interface
    Abhijit Kar
    Sudipta Mandal
    Rabindra N. Ghosh
    Tamal K. Ghosh
    Ajoy Kumar Ray
    Journal of Materials Science, 2007, 42 : 5556 - 5561
  • [45] Deformation and fracture mechanisms of Al2O3/Nb/Al2O3 composites under compression
    Zhang, ZF
    Brunner, D
    Scheu, C
    Rühle, M
    ZEITSCHRIFT FUR METALLKUNDE, 2005, 96 (01): : 62 - 70
  • [46] Microstructure and modifications of Cu/Al2O3 interfaces
    Scheu, C
    Stein, W
    Klein, S
    Wagner, T
    Tomsia, AP
    Rühle, M
    ZEITSCHRIFT FUR METALLKUNDE, 2001, 92 (07): : 707 - 711
  • [47] Effects of sulfur on the fatigue and fracture resistance of interfaces between γ-Ni(Cr) and α-Al2O3
    F. G. Gaudette
    S. Suresh
    A. G. Evans
    Metallurgical and Materials Transactions A, 2000, 31 : 1977 - 1983
  • [48] Effect of Al2O3 on mechanical properties of Ti3SiC2/Al2O3 composite
    Wang, HJ
    Jin, ZH
    Miyamoto, Y
    CERAMICS INTERNATIONAL, 2002, 28 (08) : 931 - 934
  • [49] Effects of sulfur on the fatigue and fracture resistance of interfaces between γ-Ni(Cr) and α-Al2O3
    Gaudette, FG
    Suresh, S
    Evans, AG
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2000, 31 (08): : 1977 - 1983
  • [50] Strain Engineering for the Kapitza Resistance of the ZrO2/α-Al2O3 and YSZ/α-Al2O3 Interfaces
    Xue, Yixuan
    Jiang, Jin-Wu
    ACTA MECHANICA SOLIDA SINICA, 2022, 35 (01): : 101 - 112