摘要
The behaviour of specular reflectance of cobalt oxides on metal has been studied theoretically (CoO/Co system) and experimentally (Co3O4/CO system; the thin films are obtained by chemical spray pyrolysis) in the infrared region. CoO may be identified by a LO mode at 585 cm-1 and by a TO mode at 345 cm-1 . Co3O4 is characterized by five bands respectively at 690 (LO), 660 (TO), 605 (LO), 560 (TO) and 390 cm-1. These experimental results allow the characterization of CoO and Co3O4 grown on metal during the initial stages of thermal oxidation (400-750-degrees-C). For film thicknesses in the range 10-1000 nm, the amounts of CoO and Co3O4 in the duplex structure layers may be estimated by FTIR reflectance spectroscopy. FTIR and XRD studies reveal a cyclic behaviour in the growth of the Co3O4/COO/CO system.
引用
收藏
页码:477 / 483
页数:7
相关论文
共 50 条
  • [31] INITIAL-STAGES OF EUTECTIC HARDENING
    PODOLINSKII, VV
    DRYKIN, VG
    [J]. ZHURNAL FIZICHESKOI KHIMII, 1986, 60 (10): : 2596 - 2598
  • [32] SI EJECTION AND REGROWTH DURING THE INITIAL-STAGES OF SI(001) OXIDATION
    CAHILL, DG
    AVOURIS, P
    [J]. APPLIED PHYSICS LETTERS, 1992, 60 (03) : 326 - 328
  • [33] INITIAL-STAGES OF FE(110) OXIDATION AT 300 K - KINETICS AND STRUCTURE
    WIGHT, A
    CONDON, NG
    LEIBSLE, FM
    WORTHY, G
    HODGSON, A
    [J]. SURFACE SCIENCE, 1995, 331 : 133 - 137
  • [34] DETERMINATION OF KINETIC-PARAMETERS FROM THE INITIAL-STAGES OF ETHYLBENZENE OXIDATION
    GAGARINA, AB
    DANOCZY, E
    EMANUEL, NM
    GAL, D
    [J]. MAGYAR KEMIAI FOLYOIRAT, 1979, 85 (12): : 529 - 532
  • [35] EMISSION PHENOMENA ON INITIAL-STAGES OF MAGNESIUM THIN-FILMS OXIDATION
    IVANKIV, LI
    PENTSAK, AM
    TKHIR, SG
    [J]. IZVESTIYA AKADEMII NAUK SSSR SERIYA FIZICHESKAYA, 1985, 49 (09): : 1850 - 1854
  • [36] SURFACE ELECTRONIC-STRUCTURE FOR THE INITIAL-STAGES OF ELECTROCHEMICAL OXIDATION OF ZINC
    BUCHHOLZ, JC
    [J]. BULLETIN OF THE AMERICAN PHYSICAL SOCIETY, 1979, 24 (03): : 279 - 279
  • [37] BURNS OF FACE IN INITIAL-STAGES
    PONS, J
    MONTEIL, R
    GUILBAUD, JL
    PASTUREL, A
    [J]. MEDECINE ET ARMEES, 1977, 5 (05): : 391 - 398
  • [38] LEED-AES STUDY OF INITIAL-STAGES OF OXIDATION OF FE(001)
    SIMMONS, GW
    DWYER, DJ
    [J]. SURFACE SCIENCE, 1975, 48 (02) : 373 - 392
  • [39] INFRARED-SPECTROSCOPY STUDY OF INITIAL-STAGES OF OXIDATION OF HYDROGEN-TERMINATED SI SURFACES STORED IN AIR
    NIWANO, M
    KAGEYAMA, J
    KURITA, K
    KINASHI, K
    TAKAHASHI, I
    MIYAMOTO, N
    [J]. JOURNAL OF APPLIED PHYSICS, 1994, 76 (04) : 2157 - 2163
  • [40] AN AUGER-ELECTRON SPECTROSCOPY (AES) STUDY OF THE INITIAL-STAGES OF OXIDATION OF THE SINGLE-CRYSTAL BE (0001) SURFACE
    FOWLER, DE
    BLAKELY, JM
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1982, 20 (04): : 930 - 933