AGING ENHANCEMENT IN WELD JOINT OF TI-15V-3CR-3SN-3AL ALLOY

被引:0
|
作者
SHIRASUNA, Y
NOZUE, A
OKUBO, T
机构
[1] Sophia Univ, Tokyo
关键词
TITANIUM ALLOY; WELDING; AGING; MICROSTRUCTURE; THERMOMECHANICAL TREATMENT;
D O I
10.2320/jinstmet1952.59.9_933
中图分类号
学科分类号
摘要
Weld joint is locally deformed plastically and simultaneously restored at a high temperature after welding, and subsequently cooled to room temperature. Its singular thermomechanical hysteresis of the weld joint may affect aging behavior. Ti-15V-3Cr-3Sn-3Al alloys have showed aging enhancement in the weld joint. In the present study, we clarify the aging enhancement mechansim of this alloy on the base of the thermomechanical processing. A distinctive microstructure has existed in the weld joint after the welding and the subsequent cooling. Fringe-type microstructures of plate and bulk configuration may be created by local plastic deformation due to thermal stress after welding and by freezing of a solute atom atmosphere in the vicinity of edge dislocation component on cooling. Its distinctive microstructures have promoted the aging because of preferential sites for or precipitation. From the present results, a thermomechanical treatment has been proposed to obtain a high strength of this alloy by more short aging time.
引用
收藏
页码:933 / 938
页数:6
相关论文
共 50 条
  • [41] TRANSMISSION ELECTRON-MICROSCOPY OF (332)[113]-DEFORMATION TWIN IN TI-15V-3CR-3SN-3AL ALLOY
    FURUHARA, T
    KISHIMOTO, K
    MAKI, T
    MATERIALS TRANSACTIONS JIM, 1994, 35 (12): : 843 - 850
  • [42] EFFECT OF QUENCHED-IN VACANCIES ON AGED MICROSTRUCTURES IN TI-15V-3CR-3SN-3AL
    FUJII, H
    SUZUKI, HG
    MATERIALS TRANSACTIONS JIM, 1993, 34 (04): : 382 - 388
  • [43] UNRECRYSTALLIZED GRAINS APPEARING IN TI-15V-3CR-3SN-3AL HOT ROLLED SHEET
    TAKATORI, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (13): : 1633 - 1633
  • [44] WORKABILITY AND HEAT-TREATMENT CHARACTERISTICS OF BETA-TITANIUM ALLOY, TI-15V-3CR-3SN-3AL
    TSUMORI, Y
    MATSUMOTO, T
    KOYAMA, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (06): : 603 - 609
  • [45] Fracture Toughness of Ti-15V-3Cr-3Sn-3Al Titanium Alloy in Different Heat-Treated Conditions
    Manikandan, P.
    Kumar, K. Naresh
    Rao, G. Sudarshan
    Jha, Abhay K.
    Narayanan, P. Ramesh
    Pant, Bhanu
    Cherian, Roy M.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (06) : 1507 - 1510
  • [46] EFFECT OF BI-MODAL MICROSTRUCTURE ON FRACTURE-TOUGHNESS OF TI-15V-3CR-3SN-3AL ALLOY
    NIWA, N
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1992, 78 (03): : 493 - 499
  • [47] High-temperature oxidation of a Ti-15V-3Cr-3Sn-3Al alloy in CO2 atmosphere
    Kusabiraki, K
    Fukuda, Y
    Saji, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (03): : 132 - 137
  • [48] Microplasticity and tensile damage in Ti-15V-3Cr-3Al-3Sn alloy and Ti-15V-3Cr-3Al-3Sn/SiC composite
    Soboyejo, WO
    Rabeeh, B
    Li, Y
    Soboyejo, ABO
    Rokhlin, S
    ADVANCED METHODS IN MATERIALS PROCESSING DEFECTS, 1997, 45 : 185 - 194
  • [49] TOUGHENING IN WELD JOINT OF T-15V-3CR-3SN-3AL ALLOY WITH HEAT-TREATMENT
    SHIRASUNA, Y
    NOZUE, A
    OKUBO, T
    KURIBAYASI, K
    HORIUCHI, R
    ISHIMOTO, S
    SATO, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1991, 77 (09): : 1489 - 1494
  • [50] UNRECRYSTALLIZED GRAINS APPEARING IN Ti-15V-3Cr-3Sn-3Al HOT ROLLED SHEET.
    Niwa, Naoki
    Ito, Kunio
    Yagishita, Hiroshi
    Sato, Shunji
    Takatori, Hideo
    Sakuyama, Hideo
    Transactions of the Iron and Steel Institute of Japan, 1986, 27 (03)