ACTIVATION OF NI/AL2O3 CATALYSTS THROUGH MODIFICATION OF THE AL2O3 SUPPORT

被引:9
|
作者
LINDFORS, LP [1 ]
SMEDS, S [1 ]
机构
[1] ABO AKAD, IND CHEM LAB, SF-20500 TURKU, FINLAND
关键词
NI/AL2O3; CATALYSTS; GAMMA-ALUMINA AND THETA-ALUMINA; HYDROGENATION ACTIVITY TOF; TPD OF HYDROGEN; H-2; CHEMISORPTION;
D O I
10.1007/BF00806059
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effect of alumina pretreatment on the performance of alumina supported nickel catalysts was demonstrated in gas phase hydrogenation of toluene to methylcyclohexane. The state of the alumina was changed from pure gamma to pure theta phase through various heat treatments in air. The catalysts were prepared from vapor phase by saturating the accessible binding sites on the pretreated alumina with the nickel precursor. The highest number of active sites for hydrogenation was observed for catalysts prepared on alumina having an incomplete phase transition and a theta/gamma alumina phase ratio between 0.5 and 10. Results from temperature programmed desorption (TPD) studies revealed that a maximum in weakly chemisorbed hydrogen as well as in total amount of desorbed hydrogen was found for the same catalysts. By hydrogen chemisorption studies the total hydrogen uptake was found to correlate with the observed hydrogenation maximum. It is suggested that both the chemical and physical properties of the alumina influence the activity. An optimal metal-support interaction and structural defects on the alumina due to the phase transition can explain the observed maximum in the number of active sites and in hydrogen uptake.
引用
下载
收藏
页码:291 / 299
页数:9
相关论文
共 50 条
  • [43] Effects of Ni-Al2O3 interaction on NiMo/Al2O3 hydrodesulfurization catalysts
    Liu, Zhiwei
    Han, Wei
    Hu, Dawei
    Sun, Shuling
    Hu, Anpeng
    Wang, Zhen
    Jia, Yanzi
    Zhao, Xinqiang
    Yang, Qinghe
    JOURNAL OF CATALYSIS, 2020, 387 (387) : 62 - 72
  • [44] Influence of surface modification of alumina on bond strength in Al2O3/Al/Al2O3 joints
    Ksiazek, M
    Sobczak, N
    Mikulowski, B
    Radziwill, W
    Winiarski, B
    Wojcik, M
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (9-10) : 2513 - 2517
  • [45] Influence of surface modification of alumina on bond strength in Al2O3/Al/Al2O3 joints
    M. Ksiazek
    N. Sobczak
    B. Mikulowski
    W. Radziwill
    B. Winiarski
    M. Wojcik
    Journal of Materials Science, 2005, 40 : 2513 - 2517
  • [46] Investigation of the reaction network for the hydrodesulfurization of 4,6-dimethyldibenzothiophene over NiW/Al2O3, W/Al2O3 and Ni/Al2O3 catalysts:: Promoting effects of Ni
    Koizumi, N
    Hata, K
    Nishina, A
    Yoshida, M
    Yamada, M
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2005, 230 : U2329 - U2329
  • [47] Surface and catalytic properties of Al2O3, CuO/Al2O3 and ZnO/Al2O3 systems
    El-Nabarawy, Th.
    Attia, A.A.
    Hassan, N.A.
    Youssef, A.M.
    Adsorption Science and Technology, 1995, 12 (02):
  • [48] Mechanism for the κ-Al2O3 to the α-Al2O3 transition and the stability of κ-Al2O3 under volume expansion
    Belonoshko, AB
    Ahuja, R
    Johansson, B
    PHYSICAL REVIEW B, 2000, 61 (05): : 3131 - 3134
  • [49] Interfacial reactions in Al2O3/Ti, Al2O3/Ti3Al and Al2O3/TiAl bilayers
    Zalar, A
    Baretzky, BMM
    Hofmann, S
    Rühle, M
    Panjan, P
    THIN SOLID FILMS, 1999, 352 (1-2) : 151 - 155
  • [50] JOINING Al2O3 TO Al2O3 BY BRAZING.
    Naka, Masaaki
    Kim, Kaoru
    Okamoto, Ikuo
    Transactions of JWRI (Japanese Welding Research Institute), 1984, 13 (01): : 157 - 158