EFFECT OF FIBER COATING ON THE FRACTURE AND FATIGUE RESISTANCE OF SCS-6/TI3AL COMPOSITES

被引:17
|
作者
CHIU, HP [1 ]
YANG, JM [1 ]
机构
[1] UNIV CALIF LOS ANGELES, DEPT MAT SCI & ENGN, LOS ANGELES, CA 90024 USA
来源
ACTA METALLURGICA ET MATERIALIA | 1995年 / 43卷 / 07期
基金
美国国家科学基金会;
关键词
D O I
10.1016/0956-7151(94)00471-S
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of a Ag/Ta coating on the fracture resistance of a notched SCS-6 fiber-reinforced Ti3Al matrix composite under both static and fatigue loading was investigated. The crack propagation patterns and damage mechanisms under various loading conditions were characterized and compared with its uncoated composite counterparts. The results show that the Ag/Ta-coated composites exhibit a typical mode-I failure pattern under both static and fatigue loading, while mixed mode-I and -II failure patterns were observed in the uncoated SCS-6/Ti-25-10 composite. Under fatigue loading, crack propagation was arrested at stress intensity levels up to 34 and 45 MPa m(1/2) for Ag/Ta-coated and uncoated SCS-6/Ti-25-10 composites, respectively. Localized interfacial debonding, matrix cracking and fiber bridging in the crack wake were the responsible damage mechanisms for the Ag/Ta-coated SCS-6/Ti-25-10 composite. Extensive interfacial debonding, crack splitting and branching, however, were found to be the dominant mechanisms in the uncoated SCS-6/Ti-25-10 composite. Modifications of interfacial bond strength and morphology so as to improve the mechanical properties of the Ag/Ta-coated SCS-6/Ti-25-10 composite can be achieved by thermal exposure at 800 degrees C for up to 200 h.
引用
收藏
页码:2581 / 2587
页数:7
相关论文
共 50 条
  • [21] DAMAGE EVOLUTION OF ANGLE-PLY SCS-6/TI COMPOSITES UNDER STATIC AND FATIGUE LOADING
    WANG, PC
    JENG, SM
    CHIU, HP
    YANG, JM
    JOURNAL OF MATERIALS SCIENCE, 1995, 30 (07) : 1818 - 1826
  • [22] ELEVATED-TEMPERATURE FATIGUE BEHAVIOR OF SCS-6/TI-24AL-11NB
    NICHOLAS, T
    RUSS, SM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 153 (1-2): : 514 - 519
  • [23] Study on SCS-6/Ti-6Al-4V composite
    Zeng, LY
    Zhao, YQ
    Zhou, L
    Vassel, A
    14TH CONGRESS OF INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING, VOLS 1 and 2, PROCEEDINGS, 2004, : 110 - 112
  • [24] EFFECT OF COATING THICKNESS ON THE STRENGTH OF SCS-6 SIC FIBERS
    RITTER, AM
    DUPREE, PL
    SCRIPTA METALLURGICA ET MATERIALIA, 1992, 27 (07): : 827 - 831
  • [25] Kinetics and mechanism of interfacial reaction in SCS-6 SiC continuous fiber-reinforced Ti-Al intermetallic matrix composites
    吕祥鸿
    杨延清
    马志军
    刘翠霞
    陈彦
    艾云龙
    TransactionsofNonferrousMetalsSocietyofChina, 2006, (01) : 77 - 83
  • [26] Fatigue crack growth in a Tiβ21s/SCS-6 composite
    Liu, J
    Bowen, P
    ACTA MATERIALIA, 2002, 50 (17) : 4205 - 4218
  • [27] FATIGUE BEHAVIOR OF SILICON-CARBIDE REINFORCED TITANIUM (TI/SCS-6) METAL-MATRIX COMPOSITES
    LIAW, PK
    DIAZ, ES
    CHIANG, KT
    LOH, DH
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (10): : 1643 - 1648
  • [28] Micromechanical modelling of SCS-6 fibre reinforced Ti-6Al-4V under transverse tension - Effect of fibre coating
    Li, DS
    Wisnom, MR
    JOURNAL OF COMPOSITE MATERIALS, 1996, 30 (05) : 561 - 588
  • [29] Fatigue strength of SCS-6 bridging fibers in titanium metal matrix composites
    Tamin, MN
    Ghonem, H
    PROCESSING AND FABRICATION OF ADVANCED MATERIALS VI, VOLS 1 & 2, 1998, : 691 - 702
  • [30] THE EFFECT OF FIBER-MATRIX REACTIONS ON THE INTERFACE PROPERTIES IN A SCS-6/TI-24AL-11NB COMPOSITE
    CANTONWINE, PE
    WADLEY, HNG
    COMPOSITES ENGINEERING, 1994, 4 (01): : 67 - 80