共 50 条
- [2] Effect of cold drawing on susceptibility to hydrogen embrittlement of prestressing steel Materiaux et constructions, 1993, 26 (155): : 30 - 37
- [3] EFFECT OF COLD DRAWING ON SUSCEPTIBILITY TO HYDROGEN EMBRITTLEMENT OF PRESTRESSING STEEL MATERIALS AND STRUCTURES, 1993, 26 (155): : 30 - 37
- [4] Effect of residual stress profile on hydrogen embrittlement susceptibility of prestressing steel SURFACE TREATMENT IV: COMPUTER METHODS AND EXPERIMENTAL MEASUREMENTS, 1999, 3 : 83 - 92
- [5] EFFECT OF SURFACE RESIDUAL-STRESS ON HYDROGEN EMBRITTLEMENT OF PRESTRESSING STEELS BRITISH CORROSION JOURNAL, 1983, 18 (02): : 80 - 81
- [8] Hydrogen embrittlement of prestressing steels: the concept of effective stress in design MATERIALS & DESIGN, 1997, 18 (02): : 81 - 85
- [9] Hydrogen embrittlement of prestressing steels: The concept of effective stress in design Materials and Design, 1997, 18 (02): : 81 - 85