摘要
A study was carried out on the inhibition of corrosion and hydrogen embrittlement of AISI 410 stainless steel by two organic inhibitors, namely benzotriazole and benzonitrile. Tensile testing, scanning electron microscopy, weight loss measurements and potentiodynamic polarization were the techniques used for this study. Tensile tests showed that 410 steel is highly susceptible to hydrogen stress cracking. Scanning electron microscopic observations of fracture surfaces showed a brittle quasi-cleavage type of failure when the steel was hydrogen charged from 0.5 M H2SO4. Both inhibitors reduced hydrogen induced ductility loss though the fracture mode was unaltered. They showed increasing inhibition efficiencies for corrosion as well as cathodic hydrogen evolution as their concentration in H2SO4 increased from 3.9 x 10(-5) M to 8.4 x 10(-3) M. Benzonitrile was found to be a more efficient inhibitor than benzotriazole for AISI 410 stainless steel exposed to 0.5 M H2SO4.
引用
收藏
页码:383 / 389
页数:7
相关论文
共 50 条
  • [41] Fractographic studies of hydrogen embrittlement of AISI 316L austenitic stainless steel
    Herms, E
    ANNALES DE CHIMIE-SCIENCE DES MATERIAUX, 1999, 24 (4-5): : 275 - 280
  • [42] Effect of laser surface hardening on the hydrogen embrittlement of AISI 420: Martensitic stainless steel
    Mahmoudi, B.
    Torkamany, M. J.
    Aghdam, A. R. Sabour
    Sabbaghzadeh, J.
    MATERIALS & DESIGN, 2011, 32 (05): : 2621 - 2627
  • [43] INVERSE MAGNETOSTRICTIVE SENSITIVITY OF MARTENSITIC STAINLESS-STEEL AISI-410 AND ITS APPLICATION TO PRESSURE MEASUREMENTS
    ARA, K
    BRAKAS, MJ
    IEEE TRANSACTIONS ON MAGNETICS, 1975, 11 (05) : 1352 - 1354
  • [44] Effects of hydrogen on passive film and corrosion of AISI 310 stainless steel
    Yang, MZ
    Yang, Q
    Luo, JL
    CORROSION SCIENCE, 1999, 41 (04) : 741 - 745
  • [45] CORROSION POTENTIALS AND CORROSION BEHAVIOR OF AISI 304 STAINLESS-STEEL IN HIGH-TEMPERATURE WATER CONTAINING BOTH DISSOLVED HYDROGEN AND OXYGEN
    NIEDRACH, LW
    STODDARD, WH
    CORROSION, 1986, 42 (12) : 696 - 699
  • [46] TEMPERING OF AISI-403 STAINLESS-STEEL
    LIM, LC
    LAI, MO
    MA, J
    NORTHWOOD, DO
    MIAO, B
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1993, 171 (1-2): : 13 - 19
  • [47] DEGRADATION OF AN AISI 304 STAINLESS-STEEL TANK
    Torkar, Matjaz
    Paulin, Irena
    Podgornik, Bojan
    MATERIALI IN TEHNOLOGIJE, 2016, 50 (03): : 461 - 466
  • [48] THE INHIBITION OF SULFURIC-ACID CORROSION OF 410-STAINLESS-STEEL BY THIOUREAS
    AGRAWAL, R
    NAMBOODHIRI, TKG
    CORROSION SCIENCE, 1990, 30 (01) : 37 - 52
  • [49] REDUCTION OF OXIDES BY TREATMENT IN HYDROGEN OF TYPE-410L STAINLESS-STEEL POWDER
    GOLDMAN, DB
    HART, S
    GUTMANAS, EY
    MATERIALS SCIENCE AND ENGINEERING, 1985, 72 (02): : 191 - 198
  • [50] CHLORIDE STRESS-CORROSION CRACKING OF AISI-304 STAINLESS-STEEL IN AIR
    YAJIMA, M
    ARII, M
    MATERIALS PERFORMANCE, 1980, 19 (12) : 17 - 19