- [21] DECOMPOSITION OF FERRITE TO AUSTENITE IN 26-PERCENT-CR-5-PERCENT-NI STAINLESS-STEEL METAL SCIENCE, 1980, 14 (07): : 253 - 261
- [25] OXIDATION PRETREATMENT TO REDUCE CORROSION OF 20-PERCENT-CR-25-PERCENT-NI-NB STAINLESS-STEEL .2. SURFACE-MORPHOLOGY AND OXIDE CHARACTERIZATION OXIDATION OF METALS, 1988, 30 (3-4): : 231 - 254
- [26] SOLUBILITY OF NBC IN 20 PERCENT CR-25 PERCENT NI STAINLESS STEEL JOURNAL OF THE IRON AND STEEL INSTITUTE, 1967, 205 : 535 - &
- [30] STEADY-STATE CREEP OF 20-PERCENT- CR-25-PERCENT NI STAINLESS-STEEL WITH AND WITHOUT A DISPERSION OF TIN PARTICLES ACTA METALLURGICA, 1984, 32 (12): : 2149 - 2162