KINETICS OF NITRIDING IN TITANIUM BEARING AUSTENITIC STAINLESS STEEL

被引:0
|
作者
Mohandesi, J. Aghazadeh [1 ]
Nazari, A. [1 ]
机构
[1] Amirkabir Univ Technol, Dept Min & Met Engn, 424 Hafez Ave, Tehran, Iran
关键词
kinetics of nitriding; austenitic stainless steels; mathematical model;
D O I
10.1163/157361107782106320
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The kinetics of nitriding in titanium bearing austenitic stainless steels in cylindrical coordination has been investigated. Nitriding at nitrogen partial pressure of 0.5 atm and temperature from 980 degrees C up to 1160 degrees C resulted in the formation of titanium and chromium nitride and above the Cr2N solvus temperature (1100 degrees C), no chromium nitride was formed. The nitrided case may consist of up to three zones: nitrogen in solid solution, precipitation of TiN and finally mixed TiN+Cr2N precipitation. These are in consistent with the affinity of titanium and chromium towards nitrogen which has been thermodynamically justified. To assess the kinetics of nitriding, a mathematical model for nitrogen diffusion in cylindrical system has been developed via solving Fick's equation for cylindrical coordinate by numerical method. For this purpose the use has been made of the austenite stabilizing effect of nitrogen to correlate the movement of the boundary of the nitrogen stabilized austenite and plastic deformation induced martensite. Since the crystal structure of the material used in this study is of fcc type and it is nitrided in a fully annealed and unstrained state, therefore the effect of excess nitrogen on the kinetics of nitride fronts growth has been assumed as negligible. The results are in good agreement with the previous investigations. Unlike previous works, the present model takes into account the change of nitrogen diffusion coefficient due to nitrogen concentration profile and formation of titanium nitride.
引用
收藏
页码:515 / 526
页数:12
相关论文
共 50 条
  • [41] PRECIPITATION PROCESSES IN AN AUSTENITIC STAINLESS STEEL CONTAINING TITANIUM
    SINGHAL, LK
    MARTIN, JW
    JOURNAL OF THE IRON AND STEEL INSTITUTE, 1967, 205 : 947 - &
  • [42] Enthalpy measurements on a titanium modified austenitic stainless steel
    Banerjee, A
    Raju, S
    Divakar, R
    Mohandas, E
    MATERIALS LETTERS, 2005, 59 (10) : 1219 - 1222
  • [43] Duplex treatment of AISI 304 austenitic stainless steel using rf nitriding and dc reactive magnetron sputtering of titanium
    El-Hossary, F. M.
    Negm, N. Z.
    El-Rahman, A. M. Abd
    Hammad, M.
    Templier, C.
    SURFACE & COATINGS TECHNOLOGY, 2008, 202 (08): : 1392 - 1400
  • [44] Kinetics of Low Temperature Nitriding of Precipitation Hardened Stainless Steel
    Kochmanski, Pawel
    Baranowska, Jolanta
    DIFFUSION IN SOLIDS AND LIQUIDS VI, PTS 1 AND 2, 2011, 312-315 : 530 - 535
  • [45] Mechanical properties of austenitic stainless steel treated by active screen plasma nitriding
    Hoshiyama, Yasuhiro
    Mizobata, Ryoji
    Miyake, Hidekazu
    SURFACE & COATINGS TECHNOLOGY, 2016, 307 : 1041 - 1044
  • [46] NITRIDING OF AUSTENITIC STAINLESS-STEEL BY PLASMA IMMERSION ION-IMPLANTATION
    COLLINS, GA
    HUTCHINGS, R
    SHORT, KT
    TENDYS, J
    LI, X
    SAMANDI, M
    SURFACE & COATINGS TECHNOLOGY, 1995, 74-5 (1-3): : 417 - 424
  • [47] Influence of surface preparation and ion flux on the nitriding efficiency of austenitic stainless steel
    Abrasonis, G
    Rivière, JP
    Templier, C
    Muzard, S
    Pranevicius, L
    SURFACE & COATINGS TECHNOLOGY, 2005, 196 (1-3): : 279 - 283
  • [48] Further investigation of the structure and properties of austenitic stainless steel after plasma nitriding
    Menthe, E
    Rie, KT
    SURFACE & COATINGS TECHNOLOGY, 1999, 116 : 199 - 204
  • [49] Behavior of carbon in low temperature plasma nitriding layer of austenitic stainless steel
    Tsujikawa, M
    Yamauchi, N
    Ueda, N
    Sone, T
    Hirose, Y
    SURFACE & COATINGS TECHNOLOGY, 2005, 193 (1-3): : 309 - 313
  • [50] KINETICS OF HYDROGEN EVOLUTION REACTION ON AUSTENITIC STAINLESS STEEL
    BICELLI, LP
    ROMAGNAN.C
    CHIMICA & L INDUSTRIA, 1971, 53 (12): : 1128 - &