Annealing time dependence of isochronal recovery in cold-worked aluminum

被引:1
|
作者
Nakamura, K
Ohtaki, S
Hashimoto, I
Yamaguchi, H
机构
[1] TSUBANE HIGH SCH,TSUBANE,NIIGATA 95912,JAPAN
[2] SCI UNIV TOKYO,FAC SCI,DEPT PHYS,SHINJUKU KU,TOKYO 162,JAPAN
来源
关键词
D O I
10.1002/pssa.2211520208
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Wire drawn aluminum specimens of about 0.2 mm diameter are deformed by about 16% at 4.2 K. An isochronal annealing experiment of electrical resistivity for 1, 3, or 10 min after the deformation is carried out every 5 K temperatures ranging from 30 to 150 K. The recovery sub-peaks appear at around 75 and 90 K and are shifted toward the lower temperature with increasing annealing time. The observed differential isochronal recovery curves give support to a model in which excess vacancies induced by the deformation annihilate at the jogs.
引用
收藏
页码:393 / 403
页数:11
相关论文
共 50 条