共 50 条
- [31] The rate of reaction of solid iron with oxidized “FeO”-CaO-SiO2-Al2O3 slags at 1360 °C—the chemical diffusivity of iron oxide Metallurgical and Materials Transactions B, 1999, 30 : 465 - 472
- [32] The rate of reaction of solid iron with oxidized "FeO"-CaO-SiO2-Al2O3 slags at 1360 °C -: the chemical diffusivity of iron oxide METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1999, 30 (03): : 465 - 472
- [33] Wettability of Solid Metals by Molten CaO-SiO2-Al2O3 Slag METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2008, 39 (05): : 681 - 689
- [34] Wettability of Solid Metals by Molten CaO-SiO2-Al2O3 Slag Metallurgical and Materials Transactions B, 2008, 39 : 681 - 689
- [36] Indium distribution between FeO-CaO-SiO2 slags and lead bullion at 1200 degrees C TRANSACTIONS OF THE INSTITUTIONS OF MINING AND METALLURGY SECTION C-MINERAL PROCESSING AND EXTRACTIVE METALLURGY, 2007, 116 (02): : 133 - 138
- [38] FOAMING INDEX OF CaO-SiO2-FeO-MgO SLAG SYSTEM ADVANCES IN MOLTEN SLAGS, FLUXES, AND SALTS, 2016, : 607 - 615
- [39] Effect of Initial FeO Content and CaO:SiO2 Ratio on the Reduction Smelting Kinetics of the CaO-SiO2-MgOsatd.-FeO Slag System METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2018, 49 (01): : 291 - 303
- [40] Effect of Initial FeO Content and CaO:SiO2 Ratio on the Reduction Smelting Kinetics of the CaO-SiO2-MgOsatd.-FeO Slag System Metallurgical and Materials Transactions B, 2018, 49 : 291 - 303