- [21] CREEP DEFORMATION IN 20 PERCENT CR-35 PERCENT NI STEEL [J]. JERNKONTORETS ANNALER, 1971, 155 (07): : 363 - &
- [22] PRECIPITATION IN A 20 PERCENT CR - 25 PERCENT NI STEEL STABILIZED WITH NIOBIUM [J]. JOURNAL OF THE IRON AND STEEL INSTITUTE, 1965, 203 : 398 - &
- [23] ANALYTICAL ELECTRON-MICROSCOPY OF A SELECTIVE OXIDE SCALE FORMED ON 20-PERCENT-CR-25-PERCENT-NI-NB STAINLESS-STEEL [J]. OXIDATION OF METALS, 1984, 22 (5-6): : 291 - 306
- [24] INTERPRETATION OF CREEP IN A 25CR-20NI AUSTENITIC STAINLESS-STEEL [J]. KOVOVE MATERIALY-METALLIC MATERIALS, 1984, 22 (04): : 462 - 484
- [27] DECOMPOSITION OF FERRITE TO AUSTENITE IN 26-PERCENT-CR-5-PERCENT-NI STAINLESS-STEEL [J]. METAL SCIENCE, 1980, 14 (07): : 253 - 261
- [28] OXIDATION BEHAVIOR OF 20-PERCENT CR 25-PERCENT NI-NB STABILIZED STAINLESS-STEEL IN CO2 ENVIRONMENTS [J]. OXIDATION OF METALS, 1984, 21 (3-4): : 187 - 203
- [30] NBC PRECIPITATION IN A 20 PERCENT CR - 25 PERCENT NI - 1 PERCENT NB AUSTENITIC STEEL [J]. JOURNAL OF THE IRON AND STEEL INSTITUTE, 1970, 208 : 391 - +