TENSILE BEHAVIOR OF THE L12 COMPOUND AL67TI25CR8

被引:31
|
作者
KUMAR, KS
BROWN, SA
机构
[1] Martin Marietta Laboratories, Baltimore
来源
ACTA METALLURGICA ET MATERIALIA | 1992年 / 40卷 / 08期
关键词
D O I
10.1016/0956-7151(92)90178-H
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Temperature-related variations in tensile yield strength and ductility were studied on cast, homogenized and isothermally forged Al67Ti25Cr8. Yield strength dropped discontinuously between 623 K and 773 K and then decreased gradually with increasing temperature. Below 623 K, fracture occurred prior to macroscopic yielding. Ductility decreased from 0.2% at 623 K to zero at 773 K, but increased again at higher temperatures. At 1073 K, an elongation of approximately 19% was obtainable, and ultimate tensile strength and localized necking were observed. Fracture surfaces and deformed microstructures were examined. The 1073 K tensile specimen that exhibited approximately 19% elongation showed grain boundary serrations and some evidence of recrystallization (likely dynamic) although fracture occurred predominantly via an intergranular mode.
引用
收藏
页码:1923 / 1932
页数:10
相关论文
共 50 条