Experimental study on strength properties, fracture patterns, and permeability behaviors of sandstone containing two filled fissures under triaxial compression

被引:0
|
作者
Tingchun Li
Yiteng Du
Qingwen Zhu
Jinlin Ran
Hao Zhang
Xueyang Xing
机构
[1] Shandong University of Science and Technology,Shandong Key Laboratory of Civil Engineering Disaster Prevention and Mitigation
[2] Binzhou University,Department of Architectural Engineering
关键词
Sandstone; Filled fissures; Hydromechanical coupling; Mechanical property; Failure behavior; Permeability evolution;
D O I
暂无
中图分类号
学科分类号
摘要
Rock masses generally contain many fissures filled with weak materials. At present, the interaction mechanisms of crack coalescence and seepage in rock with filled fissures are still poorly understood. Therefore, this study conducts systematic laboratory tests on sandstone samples with two filled fissures under hydromechanical coupling conditions. The influences of the fissures, filling, ligament length, and bridge angle on the strength, fracture pattern, and permeability are explored. The results show that the strength properties of the sandstone are weakened more significantly by fissures than by water pressure. The increase of strength properties induced by the fillings is more remarkable in the samples with either a longer ligament length or a lower bridge angle. Unlike for mud filling, for sand filling, most of the sand particles in the fissures are crushed after loading, reflecting that the bearing capacity of the sand filling is fully utilized. Thus, sand filling generally has a greater effect on the strength properties than mud filling does. Furthermore, the failure of double-fissure sandstone can be divided into five modes. With the exception of the samples with a high bridge angle, the samples undergo failure modes that change with the existence of fillings, and for samples with a long ligament length or a low bridge angle, the change is more sensitive to the filling type. The weakening effect of fillings on permeability is associated with the failure mode, and it is more remarkable in samples with the “wing cracks + indirect crack coalescence” or “wing cracks + direct crack coalescence” failure modes than in other samples.
引用
收藏
页码:5921 / 5938
页数:17
相关论文
共 50 条
  • [41] An experimental study on fracture mechanical behavior of rock-like materials containing two unparallel fissures under uniaxial compression
    Huang, Yan-Hua
    Yang, Sheng-Qi
    Tian, Wen-Ling
    Zeng, Wei
    Yu, Li-Yuan
    ACTA MECHANICA SINICA, 2016, 32 (03) : 442 - 455
  • [42] An experimental study on fracture mechanical behavior of rock-like materials containing two unparallel fissures under uniaxial compression
    Yan-Hua Huang
    Sheng-Qi Yang
    Wen-Ling Tian
    Wei Zeng
    Li-Yuan Yu
    Acta Mechanica Sinica, 2016, 32 : 442 - 455
  • [43] Fracture evolution characteristics of sandstone containing double fissures and a single circular hole under uniaxial compression
    Chen Minliang
    Jing Hongwen
    Ma Xiujun
    Su Haijian
    Du Mingrui
    Zhu Tantan
    International Journal of Mining Science and Technology, 2017, 27 (03) : 499 - 505
  • [44] Experimental study on permeability properties of damaged sandstone specimen in compression
    Qin Yue-ping
    Luo Wei
    Liu Wei
    Wang Xiao-jun
    Hao Yong-jiang
    ISMSSE 2011, 2011, 26
  • [45] Fracture evolution characteristics of sandstone containing double fissures and a single circular hole under uniaxial compression
    Chen Minliang
    Jing Hongwen
    Ma Xiujun
    Su Haijian
    Du Mingrui
    Zhu Tantan
    INTERNATIONAL JOURNAL OF MINING SCIENCE AND TECHNOLOGY, 2017, 27 (03) : 499 - 505
  • [46] An Experimental Study of the Fracture Coalescence Behaviour of Brittle Sandstone Specimens Containing Three Fissures
    S. Q. Yang
    D. S. Yang
    H. W. Jing
    Y. H. Li
    S. Y. Wang
    Rock Mechanics and Rock Engineering, 2012, 45 : 563 - 582
  • [47] An Experimental Study of the Fracture Coalescence Behaviour of Brittle Sandstone Specimens Containing Three Fissures
    Yang, S. Q.
    Yang, D. S.
    Jing, H. W.
    Li, Y. H.
    Wang, S. Y.
    ROCK MECHANICS AND ROCK ENGINEERING, 2012, 45 (04) : 563 - 582
  • [48] Experimental Study on Deformation and Strength Characteristics of Interbedded Sandstone with Different Interlayer Thickness under Uniaxial and Triaxial Compression
    Li, Huigui
    Wang, Jun
    Li, Huamin
    Wei, Shengjie
    Li, Xiaolong
    PROCESSES, 2022, 10 (02)
  • [49] Experimental study on deformation, peak strength and crack damage behavior of hollow sandstone under conventional triaxial compression
    Yang, Sheng-Qi
    ENGINEERING GEOLOGY, 2016, 213 : 11 - 24
  • [50] Experimental and analytical investigations on strength and deformation behaviour of red sandstone under conventional triaxial compression
    Shi, Hai-Ling
    Zhao, Lun-Yang
    Zhu, Qi-Zhi
    EUROPEAN JOURNAL OF ENVIRONMENTAL AND CIVIL ENGINEERING, 2023, 27 (13) : 3951 - 3965