Tungsten content and grain boundary misorientation angle effect on crack blunting in nanocrystalline Ni-W alloy

被引:0
|
作者
Yanjie Zhao
Jianqiu Zhou
机构
[1] Nanjing Tech University,Department of Mechanical and power Engineering
[2] Wuhan Institute of Technology,School of Mechanical & Electrical Engineering
来源
关键词
Crack blunting; Fracture toughness; Dislocations; Grain boundary; Critical penetration stress; Nanomechanics; Modeling; Simulation;
D O I
暂无
中图分类号
学科分类号
摘要
The effect of tungsten (W) content and grain boundary misorientation angle (GBMOA) on crack blunting of nanocrystalline Ni-W alloy (20–100 nm) is researched theoretically, considering the coupled effects of dislocations and grain boundaries (GBs). In our proposed model, W atoms are clustered in the dislocation free region (DFZ), impeding dislocation slip, and W additions lead to GB segregation so that the boundary energy is reduced. The dislocations emitted from the crack tip are stopped at or/and penetrated through GBs, which depends on the total force acting on the dislocations as well as the critical penetration stress. The critical penetration stress is bound up with GB energy and residual Burgers vector. The number of dislocations emitted from the crack tip and penetrated through GB is calculated by using W content and GBMOA. The results show that an increase in W content decreases the critical penetration stress and increases the number of dislocations emitted from the crack tip. The critical stress intensity factors by considering the interactions between dislocations and GBs are larger than those of dislocations stayed at GBs. It is demonstrated that crack blunting depends significantly on both W content and GBMOA.
引用
下载
收藏
相关论文
共 50 条
  • [31] Effect of polarization type on properties of Ni-W nanocrystalline electrodeposits
    Kabi, S.
    Raeissi, K.
    Saatchi, A.
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2009, 39 (08) : 1279 - 1285
  • [32] The effect of nanocrystalline Ni-W coating on the tensile properties of copper
    Panagopoulos, C. N.
    Georgiou, E. P.
    Lagaris, D. A.
    Antonakaki, V.
    AIMS MATERIALS SCIENCE, 2016, 3 (02) : 324 - 338
  • [33] Effect of solute atoms on grain boundary stability of nanocrystalline Ni–Co alloy
    Xiaotong Chen
    Xuefeng Lu
    Junqiang Ren
    Hongtao Xue
    Fuling Tang
    Yutian Ding
    Journal of Materials Science, 2022, 57 : 21352 - 21362
  • [34] Isotropic magnetization response of electrodeposited nanocrystalline Ni-W alloy nanowire arrays
    Ohgai, Takeshi
    Fujimaru, Takafumi
    Tanaka, Yoshitomo
    JOURNAL OF APPLIED ELECTROCHEMISTRY, 2014, 44 (02) : 301 - 307
  • [35] Corrosion and tribological properties of nanocrystalline pulse electrodeposited Ni-W alloy coatings
    Druga, J.
    Kasiarova, M.
    Dobrocka, E.
    Zemanova, M.
    TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 2017, 95 (01): : 39 - 45
  • [36] Determination of five-parameter grain boundary characteristics in nanocrystalline Ni-W by scanning precession electron diffraction tomography
    Harrison, Patrick
    Das, Saurabh Mohan
    Goncalves, William
    da Silva, Alessandra
    Chen, Xinren
    Vigano, Nicola
    Liebscher, Christian H.
    Ludwig, Wolfgang
    Zhou, Xuyang
    Rauch, Edgar F.
    ULTRAMICROSCOPY, 2024, 267
  • [37] Grain boundary relaxation strengthening of nanocrystalline Ni–W alloys
    Timothy J. Rupert
    Jason R. Trelewicz
    Christopher A. Schuh
    Journal of Materials Research, 2012, 27 : 1285 - 1294
  • [38] Structural investigations on nanocrystalline Ni-W alloy films by transmission electron microscopy
    Klimenkov, M.
    Haseeb, A. S. M. A.
    Bade, K.
    THIN SOLID FILMS, 2009, 517 (24) : 6593 - 6598
  • [39] Thick grain boundary induced strengthening in nanocrystalline Ni alloy
    Ding, Jie
    Neffati, D.
    Li, Qiang
    Su, R.
    Li, Jin
    Xue, S.
    Shang, Z.
    Zhang, Y.
    Wang, H.
    Kulkarni, Y.
    Zhang, X.
    NANOSCALE, 2019, 11 (48) : 23449 - 23458
  • [40] A comparison of heat treatment effect on structural and tribological properties of tungsten rich Ni-W and Ni-W-P alloy coatings
    Srivastava C.
    Khare N.
    Limaye P.K.
    Mishra S.C.
    Singh V.
    Kumar S.
    Ghosh S.K.
    Tribology International, 2024, 198