Hot Corrosion Behavior of Cr2AlC MAX Phase Coating on Inconel 738LC Subjected to V2O5 + Na2SO4

被引:0
|
作者
Fatemeh Zakeri-Shahroudi
Behrooz Ghasemi
Hassan Abdolahpour
Mansour Razavi
机构
[1] Semnan University,Department of Materials Science Engineering
[2] Material and Energy Research Center of Karaj,Department of Ceramic
来源
Oxidation of Metals | 2022年 / 97卷
关键词
Cr; AlC; Hot corrosion; MAX phase; Superalloys; Spark plasma sintering;
D O I
暂无
中图分类号
学科分类号
摘要
In this research work, the in situ Cr2AlC MAX phase was coated on IN-738LC by utilizing the spark plasma sintering operation. The aim of this study was to investigate the hot corrosion behavior of a coating that has been exposed to a mixture of Na2SO4 and V2O5 salts at 900 °C. The XRD pattern indicated the formation of Cr2O3, α–Al2O3 and mixed oxide (Cr, Al)2O3, which suggested formation of Al2O3–Cr2O3 solid solution, on the all of the samples. After being exposed to the salts, plate-like, coral-like, and fractured plate-like morphologies were found with the corrosion products. When the hot corrosion time was increased to 30 h, the oxide layer thickness increased; however, after 40 h, the layer thickness decreased from 50 to 40 µm because of cracks in the sample and spallation of the oxide layer. This was shown by the FESEM images of the sample cross-sectional area.
引用
收藏
页码:359 / 369
页数:10
相关论文
共 50 条
  • [21] Severe Hot Corrosion of the Superalloy IN718 in Mixed Salts of Na2SO4 and V2O5 at 700 °C
    Dhananjay Pradhan
    Girija Shankar Mahobia
    Kausik Chattopadhyay
    Vakil Singh
    Journal of Materials Engineering and Performance, 2018, 27 : 4235 - 4243
  • [22] Growth of YbVO4 crystals evolved from hot corrosion reactions of Yb2Zr2O7 against V2O5 and Na2SO4 + V2O5
    Li, Sa
    Liu, Zhan-Guo
    Ouyang, Jia-Hu
    APPLIED SURFACE SCIENCE, 2013, 276 : 653 - 659
  • [23] Type II Hot Corrosion Screening Tests of a Cr2AlC MAX Phase Compound
    James L. Smialek
    Simon Gray
    Oxidation of Metals, 2018, 90 : 555 - 570
  • [24] Type II Hot Corrosion Screening Tests of a Cr2AlC MAX Phase Compound
    Smialek, James L.
    Gray, Simon
    OXIDATION OF METALS, 2018, 90 (5-6): : 555 - 570
  • [25] Evolution of Microstructures on GTA Welded AISI304 subjected to hot corrosion at 700°C under Na2SO4 + V2O5 (60%)
    Sharief, Hafeez B.
    Kumar, Senthil S.
    Yeshwanth, B. K.
    Arivazhagan, N.
    Ramkumar, Devendranath K.
    Narayanan, S.
    ADVANCED STRUCTURAL AND FUNCTIONAL MATERIALS FOR PROTECTION, 2012, 185 : 84 - 86
  • [26] Hot corrosion mechanism of yttria-stabilized zirconia powder in the presence of molten Na2SO4 + V2O5 salts
    De la Roche, Jhonattan
    Manuel Alvarado-Orozco, Juan
    Toro, Alejandro
    RARE METALS, 2021, 40 (05) : 1307 - 1316
  • [27] Hot corrosion mechanism of yttria-stabilized zirconia powder in the presence of molten Na2SO4 + V2O5 salts
    Jhonattan De la Roche
    Juan Manuel Alvarado-Orozco
    Alejandro Toro
    Rare Metals, 2021, 40 : 1307 - 1316
  • [28] Hot corrosion behavior of SiC in molten Na2SO4
    Nakagawa, T
    Hara, M
    Imai, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1997, 61 (11) : 1241 - 1248
  • [29] Hot corrosion behavior of Sc2O3-Y2O3-ZrO2 thermal barrier coatings in presence of Na2SO4 + V2O5 molten salt
    Liu, Huai-fei
    Xiong, Xiang
    Li, Xiao-bin
    Wang, Ya-lei
    CORROSION SCIENCE, 2014, 85 : 87 - 93
  • [30] Hot corrosion behavior of dense CYSZ/YSZ bilayer coatings deposited by atmospheric plasma spray in Na2SO4 + V2O5 molten salts
    de la Roche, Jhonattan
    Alvarado-Orozco, Juan Manuel
    Gomez, Pablo Andres
    Cano, Irene Garcia
    Dosta, Sergi
    Toro, Alejandro
    SURFACE & COATINGS TECHNOLOGY, 2022, 432