Spark plasma sintering of Al-SiC composites with high SiC content: study of microstructure and tribological properties

被引:2
|
作者
Leszczynska-Madej, Beata [1 ]
Madej, Marcin [2 ]
Wasik, Anna [1 ]
Garbiec, Dariusz [3 ]
机构
[1] AGH Univ Sci & Technol, Fac Nonferrous Met, 30 Mickiewicza Ave, PL-30059 Krakow, Poland
[2] AGH Univ Sci & Technol, Fac Met Engn & Ind Comp Sci, 30 Mickiewicza Ave, PL-300059 Krakow, Poland
[3] Pozna Inst Technol, Lukasiewicz Res Network, 6 Ewarysta Estkowskiego St, PL-61755 Poznan, Poland
关键词
Al-SiC composites; Spark plasma sintering; X-ray analysis; Scanning electron microscopy; Tribological properties; Wear mechanisms; HIGH-VOLUME FRACTION; MECHANICAL-PROPERTIES; WEAR BEHAVIOR; PARTICLES; REINFORCEMENT; INTERFACE;
D O I
10.1007/s43452-023-00771-y
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The article presents the results of the microstructure and tribological properties of Al-xSiC composites (x = 70 and 90 wt% SiC) produced in spark plasma sintering (SPS). Due to their attractive thermal, physical, and mechanical properties, aluminum matrix composites with high-volume fractions of silicon carbide (> 50%) have become a major area of interest as a potential material for multifunctional electronic packaging and cryogenic applications. The SPS process was carried out in a vacuum atmosphere under various conditions. Composites with a density close to theoretical (96-98%) were obtained. X-ray diffraction and scanning electron microscopy with EDS analysis were used to characterize the microstructure. Mechanical properties were determined by hardness measurements and a three-point bending test. The tribological properties of the composites were determined utilizing a block-on-ring tribotester. As a criterion for wear resistance, weight loss measured under specific friction conditions, that is, depending on the type of material and the applied load, was adopted. The researched materials were characterized by an even distribution of the carbide phase in the matrix. Composites with the highest SiC phase content (90 wt%) had higher hardness (2537 HV1) and flexural strength (242 +/- 15 MPa) with worse wear resistance at the same time. The weight loss of this composite was 0.43 and 0.76% for friction under loads of 100 and 200 N, respectively, and was 360 and 270% higher than that determined for the composites with the lower content of the SiC phase (70 wt%). The wear rate was three times higher for the Al-90wt%SiC composites.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Tribological Properties of Spark Plasma Sintered Al-SiC Composites
    Leszczynska-Madej, Beata
    Madej, Marcin
    Garbiec, Dariusz
    MATERIALS, 2020, 13 (21) : 1 - 12
  • [2] Effect of sintering temperature on microstructure and selected properties of spark plasma sintered Al-SiC composites
    Leszczynska-Madej, Beata
    Garbiec, Dariusz
    Madej, Marcin
    VACUUM, 2019, 164 : 250 - 255
  • [3] Al-SiC COMPOSITES SYNTHESIZED BY THE SPARK PLASMA SINTERING METHOD (SPS)
    Garbiec, Dariusz
    Jurczyk, Mieczyslaw
    COMPOSITES THEORY AND PRACTICE, 2013, 13 (04): : 255 - 259
  • [4] THE EFFECT OF SINTERING TEMPERATURE ON MICROSTRUCTURE AND PROPERTIES OF Al-SiC COMPOSITES
    Leszczynska-Madej, B.
    ARCHIVES OF METALLURGY AND MATERIALS, 2013, 58 (01) : 43 - 48
  • [5] Effect of sintering techniques on microstructural, mechanical and tribological properties of Al-SiC composites
    Shaikh, Mohd Bilal Naim
    Aziz, Tariq
    Arif, Sajjad
    Ansari, Akhter H.
    Karagiannidis, Panagiotis G.
    Uddin, Mohammad
    SURFACES AND INTERFACES, 2020, 20
  • [6] Microstructures and mechanical properties of spark plasma sintered Al-SiC composites containing high volume fraction of SiC
    Zhang, Zhao-Hui
    Wang, Fu-Chi
    Luo, Jie
    Lee, Shu-Kui
    Wang, Lu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (27-28): : 7235 - 7240
  • [7] The effect of SiC content on the tribocorrosion performance of spark plasma sintered Al-SiC nanocomposites
    Cobbinah, P., V
    Matizamhuka, W. R.
    SN APPLIED SCIENCES, 2019, 1 (12):
  • [8] High temperature properties of Al-SiC composites
    Saigal, A
    Doherty, B
    Materials in the Automotive Industry, 2001, : 267 - 277
  • [9] Influence of microstructure and crystallographic phases on the tribological properties of SiC obtained by spark plasma sintering
    Gutierrez-Mora, F.
    Lara, A.
    Munoz, A.
    Dominguez-Rodriguez, A.
    Melandri, C.
    de Portu, G.
    WEAR, 2014, 309 (1-2) : 29 - 34
  • [10] Microstructure and mechanical properties of BAS/SiC composites sintered by spark plasma sintering
    Ma, Jingmei
    Ye, Feng
    Hua, Zhong
    MATERIALS CHARACTERIZATION, 2013, 84 : 100 - 104