A technique for experimental determination of fracture toughness and hydrogen embrittlement of pipes made of API 5L X52 steel is described. The tests were performed using arc-shaped specimens with a notch cut out from pipes under the conditions of a three-point bend. The fracture toughness was determined in terms of the J-integral and the stress intensity factor at the notch tip. The value of Kρ,c was established using the volumetric method based on the experimentally measured critical load and the results of the FEM calculation of the distribution of elastic-plastic stresses ahead of the notch tip, and Jρ,c was determined using the method of separable functions. The effect of hydrogen embrittlement was studied using electrolytically prehydrogenated specimens.
引用
收藏
页码:1558 / 1563
页数:5
相关论文
共 50 条
  • [31] Investigation of Hydrogen Embrittlement Susceptibility and Fracture Toughness Drop after in situ Hydrogen Cathodic Charging for an X65 Pipeline Steel
    Kyriakopoulou, Helen P.
    Karmiris-Obratanski, Panagiotis
    Tazedakis, Athanasios S.
    Daniolos, Nikoalos M.
    Dourdounis, Efthymios C.
    Manolakos, Dimitrios E.
    Pantelis, Dimitrios
    MICROMACHINES, 2020, 11 (04)
  • [32] Hydrogen embrittlement of structural steels: Effect of the displacement rate on the fracture toughness of high-pressure hydrogen pre-charged samples
    Alvarez, G.
    Peral, L. B.
    Rodriguez, C.
    Garcia, T. E.
    Belzunce, F. J.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (29) : 15634 - 15643
  • [33] HYDROGEN EMBRITTLEMENT AND GRAIN-BOUNDARY FRACTURE
    ROBERTSON, IM
    TABATA, T
    WEI, W
    HEUBAUM, F
    BIRNBAUM, HK
    SCRIPTA METALLURGICA, 1984, 18 (08): : 841 - 846
  • [34] Mechanisms of hydrogen embrittlement and fracture of nanocrystalline materials
    Vlasov N.M.
    Chelyapina O.I.
    Russian Metallurgy (Metally), 2017, 2017 (4) : 245 - 249
  • [35] FRACTURE OF STEEL AT DIFFERENT STAGES OF HYDROGEN EMBRITTLEMENT
    SAVCHENKOV, EA
    SVETLICHKIN, AF
    METAL SCIENCE AND HEAT TREATMENT, 1980, 22 (11-1) : 871 - 876
  • [36] A FRACTURE TOPOGRAPHICAL FEATURE CHARACTERISTIC OF HYDROGEN EMBRITTLEMENT
    CRAIG, BD
    CORROSION, 1981, 37 (09) : 530 - 532
  • [37] HYDROGEN EMBRITTLEMENT AND GRAIN BOUNDARY FRACTURE.
    Robertson, I.M.
    Tabata, T.
    Wei, W.
    Heubaum, F.
    Birnbaum, H.K.
    1986, : 717 - 722
  • [38] The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel
    Nagao, Akihide
    Smith, Cynthia D.
    Dadfarnia, Mohsen
    Sofronis, Petros
    Robertson, Ian M.
    ACTA MATERIALIA, 2012, 60 (13-14) : 5182 - 5189
  • [39] EFFECT OF NOTCHES AND MICROSTRUCTURE ON THE FRACTURE-TOUGHNESS OF TIAL-BASED ALLOYS
    PU, ZJ
    WU, KH
    SHI, J
    ZOU, D
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 192 : 347 - 355
  • [40] On the Effect of Hydrogen on the Fracture Toughness of Steel
    Y. Kim
    Y. J. Chao
    Marty J. Pechersky
    Michael J. Morgan
    International Journal of Fracture, 2005, 134 : 339 - 347