Stability of single-wall carbon nanotubes under hydrothermal conditions

被引:0
|
作者
S. Srikanta Swamy
Jose Maria Calderon-Moreno
Masahiro Yoshimura
机构
[1] Research Institute for Solvothermal Technology,Center for Materials Design
[2] Materials and Structures Laboratory,undefined
[3] Tokyo Institute of Technology,undefined
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The stability of single-wall carbon nanotubes under hydrothermal conditions (100 MPa pressure, from 30 min to 48 h in the temperature range from 200 to 800 °C) has been investigated. The resultant products were characterized by Raman spectroscopy, x-ray diffraction, and transmission electron microscopy. The stability range of single-wall carbon nanotubes (SWCNTs) under hydrothermal conditions suggests that they, similar to fullerenes, can only survive mild and short-term treatment in high-temperature, high-pressure water. SWCNTs gradually transform into multiwall carbon nanotubes (MWCNTs) and polyhedral graphitic nanoparticules. After 48 h at 750 °C only the Raman spectra characteristic of graphitic carbon were observed. Transmission electron microscopy revealed that after 800 °C and 48 h of treatment SWCNTs fully transformed into MWCNTs and polyhedral carbon nanoparticles.
引用
收藏
页码:734 / 737
页数:3
相关论文
共 50 条
  • [31] Ferromagnetic semiconductor single-wall carbon nanotubes
    Moradian, R
    Fathalian, A
    NANOTECHNOLOGY, 2006, 17 (08) : 1835 - 1842
  • [32] Bandgap renormalization in single-wall carbon nanotubes
    Chunhui Zhu
    Yujie Liu
    Jieying Xu
    Zhonghui Nie
    Yao Li
    Yongbing Xu
    Rong Zhang
    Fengqiu Wang
    Scientific Reports, 7
  • [33] Dielectric function of single-wall carbon nanotubes
    Margulis, VA
    Gaiduk, EA
    CHEMICAL PHYSICS LETTERS, 2001, 341 (1-2) : 16 - 22
  • [34] Mechanically Interlocked Single-Wall Carbon Nanotubes**
    de Juan, Alberto
    Pouillon, Yann
    Ruiz-Gonzalez, Luisa
    Torres-Pardo, Almudena
    Casado, Santiago
    Martin, Nazario
    Rubio, Angel
    Perez, Emilio M.
    ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2014, 53 (21) : 5394 - 5400
  • [35] Opening and closing of single-wall carbon nanotubes
    Geng, HZ
    Zhang, XB
    Mao, SH
    Kleinhammes, A
    Shimoda, H
    Wu, Y
    Zhou, O
    CHEMICAL PHYSICS LETTERS, 2004, 399 (1-3) : 109 - 113
  • [36] Effect of oxidation on single-wall carbon nanotubes
    Nagasawa, S
    Yudasaka, M
    Hirahara, K
    Ichihashi, T
    Iijima, S
    CHEMICAL PHYSICS LETTERS, 2000, 328 (4-6) : 374 - 380
  • [37] Thickness of graphene and single-wall carbon nanotubes
    Huang, Y.
    Wu, J.
    Hwang, K. C.
    PHYSICAL REVIEW B, 2006, 74 (24)
  • [38] The intrinsic stiffness of single-wall carbon nanotubes
    Wu, J.
    Peng, J.
    Hwang, K. C.
    Song, J.
    Huang, Y.
    MECHANICS RESEARCH COMMUNICATIONS, 2008, 35 (1-2) : 2 - 9
  • [39] SINGLE-WALL CARBON NANOTUBES PURIFICATION AND OXIDATION
    Ciobotaru, Constantin-Claudiu
    Damian, Celina Maria
    Iovu, Horia
    UNIVERSITY POLITEHNICA OF BUCHAREST SCIENTIFIC BULLETIN SERIES B-CHEMISTRY AND MATERIALS SCIENCE, 2013, 75 (02): : 55 - 66
  • [40] Structure modification of single-wall carbon nanotubes
    Zhang, Y
    Shi, Z
    Gu, Z
    Iijima, S
    CARBON, 2000, 38 (15) : 2055 - 2059