The mechanical strength of solid oxide fuel cell (SOFC) components is one of the key issues for determining their performance and reliability. A minimum strength is required for the handling of these components in manufacturing, namely in relation to the application of the electrode or electrolyte coatings, the application of the current collection metals and the construction of the stack. Small tubular SOFCs have been found to have excellent thermal shock properties and low-cost of fabrication through traditional extrusion techniques. The mechanical integrity of the small, thin walled, tubular ceramics could be tested using traditional 3 or 4-point bending techniques, however these techniques are liable to cause failure by crushing the tube wall. Thus, a more reliable method for realizing the strength of small thin walled tubes is to pressurize the inside volume and obtain the strength value at which the tube bursts under the internal pressure. A custom burst-test instrument was constructed to obtain the average strength value of differing types of small ceramic tubes. The mechanical properties of 8 mol% yttria-stabilized zirconia (8YSZ) and NiO-YSZ tubes were investigated and are discussed. An average burst strength of 97 ± 28 MPa was observed for 8YSZ electrolyte tubes and 72 ± 23 MPa and 70 ± 16 MPa for as-sintered and reduced anode support tubes, respectively.
引用
收藏
页码:4811 / 4816
页数:5
相关论文
共 50 条
  • [41] Preparation and properties of small diameter tubular solid oxide fuel cells for rapid start-up
    Kilbride, IP
    JOURNAL OF POWER SOURCES, 1996, 61 (1-2) : 167 - 171
  • [42] Implications for Using Biogas as a Fuel Source for Solid Oxide Fuel Cells: Internal Dry Reforming in a Small Tubular Solid Oxide Fuel Cell
    John Staniforth
    R. Mark Ormerod
    Catalysis Letters, 2002, 81 : 19 - 23
  • [43] Implications for using biogas as a fuel source for solid oxide fuel cells: internal dry reforming in a small tubular solid oxide fuel cell
    Staniforth, J
    Ormerod, RM
    CATALYSIS LETTERS, 2002, 81 (1-2) : 19 - 23
  • [44] Anode barrier layers for tubular solid-oxide fuel cells with methane fuel streams
    Zhu, Huayang
    Colclasure, Andrew M.
    Kee, Robert J.
    Lin, Yuanbo
    Barnett, Scott A.
    JOURNAL OF POWER SOURCES, 2006, 161 (01) : 413 - 419
  • [45] Processing and properties of advanced solid oxide fuel cells
    Stoever, Detlev
    Buchkremer, Hans Peter
    Mai, Andreas
    Menzler, Norbert H.
    Zahid, Mohsine
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 1367 - +
  • [46] Feasibility of tubular solid oxide fuel cells directly running on liquid biofuels
    Chen, Kongfa
    Zhang, Lan
    Gholizadeh, Mortaza
    Ai, Na
    Hasan, Md Mahmudul
    Mourant, Daniel
    Li, Chun-Zhu
    Jiang, San Ping
    CHEMICAL ENGINEERING SCIENCE, 2016, 154 : 108 - 118
  • [47] Anode substrate with continuous porosity gradient for tubular solid oxide fuel cells
    Chen, Long
    Yao, Mutian
    Xia, Changrong
    ELECTROCHEMISTRY COMMUNICATIONS, 2014, 38 : 114 - 116
  • [48] Operation Characteristics of Tubular Segmented-in-Series Solid Oxide Fuel Cells
    Lim, Tak-Hyoung
    Yun, Ui-Jin
    Lee, Jong-Won
    Lee, Seung-Bok
    Park, Seok-Joo
    Song, Rak-Hyun
    Shin, Dong-Ryul
    SOLID OXIDE FUEL CELLS 12 (SOFC XII), 2011, 35 (01): : 679 - 682
  • [49] Isothermal models for anode-supported tubular solid oxide fuel cells
    Bhattacharyya, Debangsu
    Rengaswamy, Raghunathan
    Finnerty, Caine
    CHEMICAL ENGINEERING SCIENCE, 2007, 62 (16) : 4250 - 4267
  • [50] Performance and thermal stress of tubular functionally graded solid oxide fuel cells
    Gari, Abdullatif A.
    Ahmed, Khaled, I
    Ahmed, Mohamed H.
    ENERGY REPORTS, 2021, 7 : 6413 - 6421