Impact of thermal oxidation parameters on micro-hardness and hot corrosion of Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr alloy

被引:0
|
作者
Fathy S. Ahmed
Mohamed A. El-Zomor
Magdy S. Abo Ghazala
Ramadan N. Elshaer
机构
[1] Tabbin Institute for Metallurgical Studies,Faculty of Science
[2] Menofia University,undefined
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Protective oxide layers on Ti-6Al-3Mo-2Nb-2Sn-2Zr-1.5Cr (TC21) alloy with equiaxed microstructure considerably influence micro-hardness and hot corrosion resistance. The present work’s thermal oxidation of TC21 alloy was performed at 600, 700, and 800 °C for 5, 20, and 50 h durations. Hot corrosion methods in NaCl and NaCl + Na2SO4 salt media were applied to raw (unoxidized) and oxidized samples at 600 and 800 °C for 50 h. Hot corrosion was conducted at 600 °C for 5 cycles with 10-h steps. The best oxide layer thickness was observed at 800 °C, which increased with increased oxidation time and temperature. The surface hardness of the oxide layer at 800 °C was 900 ± 60 HV0.05 owing to the formation of TiO2 and Al2O3 phases. Raw material hardness was 342 ± 20 HV0.05, increasing threefold due to thermal oxidation. In the case of NaCl, weight loss dominated all samples except at 800 °C for 5 h. In the case of NaCl + Na2SO4, weight gain occurred at 600 and 800 °C for 5 h. Weight loss occurred for the raw samples and those processed at 800 °C for 20 and 50 h, where the oxide layer flaked off. Surface hardness increased upon hot corrosion testing because of the formation of brittle phases, such as TiO2 and Na4Ti5O12. Samples that oxidized at 800 °C for 5 h had the highest hardness and corrosion resistance.
引用
收藏
相关论文
共 50 条
  • [41] IMPACT TOUGHNESS OF HYDROGEN CHARGED TI-6AL-2SN-4ZR-6MO ALLOY
    NIINOMI, M
    SUZUKI, K
    KOBAYASHI, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (10): : 1405 - 1412
  • [42] Static and Fatigue Characteristics of Heat-Treated Ti–6Al–3Mo–2Zr–2Sn–2Nb–1.5Cr–0.1Si Alloy
    Ramadan N. Elshaer
    M. Abdelhameed
    Khaled M. Ibrahim
    M. El-Shennawy
    A. Sobh
    Metallography, Microstructure, and Analysis, 2022, 11 : 443 - 453
  • [43] Preparation and osteoinduction of active micro-arc oxidation films on Ti-3Zr-2Sn-3Mo-25Nb alloy
    Yu Sen
    Yu Zhen-tao
    Wang, Gui
    Han Jian-ye
    Ma Xi-qun
    Dargusch, Matthew S.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (03) : 573 - 580
  • [44] Hot Deformation Behavior and Processing Map of Ti-6Al-3Nb-2Zr-1Mo Titanium Alloy
    Chen Haisheng
    Liu Xianghong
    Liu Guangfa
    Tang Xiaodong
    Feng Yong
    Li Jinshan
    Fu Hengzhi
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (04) : 900 - 905
  • [45] The corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy: Effects of HCl concentration and temperature
    Baoxian Su
    Binbin Wang
    Liangshun Luo
    Liang Wang
    Yanqing Su
    Fuxin Wang
    Yanjin Xu
    Baoshuai Han
    Haiguang Huang
    Jingjie Guo
    Hengzhi Fu
    JournalofMaterialsScience&Technology, 2021, 74 (15) : 143 - 154
  • [46] The corrosion behavior of Ti-6Al-3Nb-2Zr-1Mo alloy: Effects of HCl concentration and temperature
    Su, Baoxian
    Wang, Binbin
    Luo, Liangshun
    Wang, Liang
    Su, Yanqing
    Wang, Fuxin
    Xu, Yanjin
    Han, Baoshuai
    Huang, Haiguang
    Guo, Jingjie
    Fu, Hengzhi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 74 : 143 - 154
  • [47] Effect of laser shock peening on the corrosion properties of Ti-6Al-3Nb-2Zr-1Mo alloy
    Luo, Gaoli
    Zhang, Lingfeng
    Xiong, Yi
    Zhang, Baofeng
    Chen, Xuepeng
    Wu, Yongli
    Wang, Shubo
    Cao, Wei
    SURFACE & COATINGS TECHNOLOGY, 2022, 440
  • [48] Experimental studies on the dynamic tensile behavior of Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-Si alloy with Widmanstatten microstructure at elevated temperatures
    Gong, Xuhui
    Wang, Yu
    Xia, Yuanming
    Ge, Peng
    Zhao, Yongqing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 53 - 59
  • [49] Effect of heat treatment and silicon addition on the microstructure development of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
    Zhang, XD
    Bonniwell, P
    Fraser, HL
    Baeslack, WA
    Evans, DJ
    Ginter, T
    Bayha, T
    Cornell, B
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 343 (1-2): : 210 - 226
  • [50] Effect of Strain Hardening and Aging Processes on Microstructure Evolution, Tensile and Fatigue Properties of Cast Ti-6Al-2Sn-2Zr–2Mo-1.5Cr-2Nb-0.1Si Alloy
    Ramadan N. Elshaer
    Mostafa S. S. El-Deeb
    S. S. Mohamed
    Khaled M. Ibrahim
    International Journal of Metalcasting, 2022, 16 : 723 - 737