Simulation of tin penetration process in the surface layer of soda-lime-silica float glass

被引:0
|
作者
Qin Zhang
ZeJing Chen
ZhiXin Li
机构
[1] Tsinghua University,Key Laboratory of Thermal Science and Power Engineering of Ministry of Education, School of Aerospace
来源
关键词
float glass; tin penetration; satellite peak;
D O I
暂无
中图分类号
学科分类号
摘要
Based on the analysis of tin penetration mechanism in the float glass process, the oxidation model of stannous ion is constructed considering the oxygen activity and the redox reaction in the glass surface layer. The calculation of stannous ion’s oxidation rate makes it possible to predict both stannous and stannic ion’s concentrations independently. And it is also the necessary precondition for the numerical verification of tin penetration mechanism. Coupled diffusion simulation method is established to simulate the penetration process of both stannous and stannic ions simultaneously. The result shows that when the green glass is formed in the reducing atmosphere in tin bath, the stannic ion is accumulated at the position where oxygen activity changes sharply. Satellite peak (internal local concentration maximum) occurs in the tin concentration profile of green glass, which is quite different from that in low iron glass. Compared with gradually cooling temperature regulation, the tin penetrated shifts to greater depth and the depth and magnitude of the satellite peak also increase when reheating temperature regulation is applied. In order to reduce the amount of penetrated tin, the residual time in the high temperature region should be shortened.
引用
收藏
页码:691 / 697
页数:6
相关论文
共 50 条
  • [41] STUDIES ON CHEMICAL STRENGTHENING OF SODA-LIME-SILICA GLASS
    WARD, JB
    SUGARMAN, B
    SYMMERS, C
    GLASS TECHNOLOGY, 1965, 6 (03): : 90 - +
  • [42] Decelerated crystal growth in a soda-lime-silica glass
    Fielitz, Peter
    Cassar, Daniel R.
    Yuritsyn, Nikolay S.
    Abyzov, Alexander S.
    Fokin, Vladimir M.
    Borchardt, Guenter
    Deubener, Joachim
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2022, 596
  • [43] SODA-LIME-SILICA GLASS FOR RADIATION-DOSIMETRY
    EZZELDIN, FM
    ABDELREHIM, F
    ABDELAZIM, AA
    AHMED, AA
    MEDICAL PHYSICS, 1994, 21 (07) : 1085 - 1089
  • [44] The sub-critical indentation fracture process in soda-lime-silica glass
    Sglavo, VM
    Green, DJ
    ENGINEERING FRACTURE MECHANICS, 1996, 55 (01) : 35 - 46
  • [45] Revealing the surface structural cause of scratch formation on soda-lime-silica glass
    Roy, Barsheek
    Rosin, Andreas
    Gerdes, Thorsten
    Schaffoener, Stefan
    SCIENTIFIC REPORTS, 2022, 12 (01)
  • [46] Revealing the surface structural cause of scratch formation on soda-lime-silica glass
    Barsheek Roy
    Andreas Rosin
    Thorsten Gerdes
    Stefan Schafföner
    Scientific Reports, 12
  • [47] Weathering of the inner surface of soda-lime-silica glass containers exposed to the atmosphere
    Verita, M.
    Falcone, R.
    Sommariva, G.
    Chopinet, M. -H.
    Lehuede, P.
    GLASS TECHNOLOGY-EUROPEAN JOURNAL OF GLASS SCIENCE AND TECHNOLOGY PART A, 2009, 50 (01): : 65 - 70
  • [48] Revealing the surface structural cause of scratch formation on soda-lime-silica glass
    不详
    AMERICAN CERAMIC SOCIETY BULLETIN, 2022, 101 (03): : 18 - 18
  • [49] Flame-impingement-induced superhydrophilicity of soda-lime-silica glass surface
    Roy, Barsheek
    Schmidt, Anne
    Rosin, Andreas
    Gerdes, Thorsten
    INTERNATIONAL JOURNAL OF APPLIED GLASS SCIENCE, 2024,
  • [50] Strengthening coating based on silica nanoparticles for soda-lime-silica glass
    S. V. Es’kin
    I. D. Kosobudsky
    A. B. Zhimalov
    N. M. Ushakov
    A. N. Gribov
    Inorganic Materials, 2014, 50 : 63 - 67