Failure behavior of Cu–Ti–Zr-based bulk metallic glass alloys

被引:1
|
作者
Medhat Awad El-Hadek
Magdy Kassem
机构
[1] Suez Canal University,Department of Mechanical Design & Production, Faculty of Engineering
[2] Suez Canal University,Department of Metallurgy, Faculty of Petroleum & Mining Engineering
来源
关键词
High Resolution Transmission Electron Microscopy; Shear Band; Metallic Glass; Amorphous Alloy; High Resolution Transmission Electron Microscopy;
D O I
暂无
中图分类号
学科分类号
摘要
Microstructure fracture and mechanical properties of Cu-based bulk metallic glass alloys were investigated. Centrifugal casting into copper molds were used to manufacture basic Cu47Ti33Zr11Ni9, and modified Cu47Ti33Zr11Ni7Si1Sn1 alloys. Although the alloys show an amorphous structure, TEM images revealed the formation of nanoparticles. At room temperature compression tests reveal fracture strength of 2000 MPa, elastic modulus of 127 GPa, and 1.8% fracture strain for the unmodified basic alloy. Whereas the modified alloy exhibits a fracture strength of 2179 MPa, elastic modulus reaches 123 GPa, and 2.4% fracture strain. So, with the addition of 1 at.% Si and Sn, the fracture strength improves by 9% and the fracture strain improves by 25%, but the fracture behavior under compression conditions exhibits a conical shape similar to that produced by tensile testing of ductile alloys. A proposed fracture mechanism explaining the formation of the conical fracture surface was adopted. The formation of homogeneously distributed nano-size (2–5 nm) precipitates changes the mode of fracture of the metallic glass from single to multiple shear plane modes leading to the conical shape fracture surface morphology.
引用
收藏
页码:1127 / 1136
页数:9
相关论文
共 50 条
  • [21] Strong liquid behavior of Zr-Ti-Cu-Ni-Be bulk metallic glass forming alloys
    Busch, R
    Masuhr, A
    Bakke, E
    Johnson, WL
    STRUCTURE AND DYNAMICS OF GLASSES AND GLASS FORMERS, 1997, 455 : 369 - 374
  • [22] Tribological behaviors of Zr-based bulk metallic glass versus Zr-based bulk metallic glass under relative heavy loads
    Zhong, Hua
    Chen, Jun
    Dai, Luanyue
    Yue, Yun
    Zhang, Zhiwei
    Zhang, Xinyu
    Ma, Mingzhen
    Liu, Riping
    INTERMETALLICS, 2015, 65 : 88 - 93
  • [23] Influence of cyclic loading on the onset of failure in a Zr-based bulk metallic glass
    D. V. Louzguine-Luzgin
    L. V. Louzguina-Luzgina
    S. V. Ketov
    V. Yu. Zadorozhnyy
    A. L. Greer
    Journal of Materials Science, 2014, 49 : 6716 - 6721
  • [24] Influence of cyclic loading on the onset of failure in a Zr-based bulk metallic glass
    Louzguine-Luzgin, D. V.
    Louzguina-Luzgina, L. V.
    Ketov, S. V.
    Zadorozhnyy, V. Yu.
    Greer, A. L.
    JOURNAL OF MATERIALS SCIENCE, 2014, 49 (19) : 6716 - 6721
  • [25] Macrophage responses to a Zr-based bulk metallic glass
    Huang, Lu
    Zhang, Tao
    Liaw, Peter K.
    He, Wei
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2014, 102 (10) : 3369 - 3378
  • [26] Quasicrystal formation in a Zr-based bulk metallic glass\
    Liu, L
    Chan, KC
    Pang, GKH
    AMORPHOUS AND NANOCRYSTALLINE METALS, 2004, 806 : 113 - 118
  • [27] Serration Dynamics in a Zr-Based Bulk Metallic Glass
    Z. Wang
    J. W. Qiao
    H. J. Yang
    P. K. Liaw
    C. J. Huang
    L. F. Li
    Metallurgical and Materials Transactions A, 2015, 46 : 2404 - 2414
  • [28] Properties of vacuum-laser-welded Ti-based bulk metallic glass and Zr-based bulk metallic glass composite
    Jun, Hyun-Joon
    Yun, Chang Gun
    Joo, Jeong Hwan
    Lee, Ho Jin
    Lee, Kwang Seok
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2019, 110 (07) : 648 - 655
  • [29] Cutting Characteristics of Zr-Based Bulk Metallic Glass
    Han, D. X.
    Wang, G.
    Li, J.
    Chan, K. C.
    To, S.
    Wu, F. F.
    Gao, Y. L.
    Zhai, Q. J.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2015, 31 (02) : 153 - 158
  • [30] The onset of plasticity of a Zr-based bulk metallic glass
    Huang, Yongjiang
    Khong, J. C.
    Connolley, Thomas
    Mi, J.
    INTERNATIONAL JOURNAL OF PLASTICITY, 2014, 60 : 87 - 100