Cyclic Deformation Behavior of Fe-18Cr-18Mn-0.63N Nickel-Free High-Nitrogen Austenitic Stainless Steel

被引:0
|
作者
C. W. Shao
F. Shi
X. W. Li
机构
[1] Northeastern University,Institute of Materials Physics and Chemistry, College of Sciences
[2] Chinese Academy of Sciences,Shenyang National Laboratory for Materials Science, Institute of Metal Research
[3] Northeastern University,Key Laboratory for Anisotropy and Texture of Materials, Ministry of Education
关键词
Fatigue Life; Effective Stress; Strain Amplitude; Slip Band; Cyclic Deformation;
D O I
暂无
中图分类号
学科分类号
摘要
Cyclic deformation and damage behavior of a Ni-free high-nitrogen austenitic stainless steel with a composition of Fe-18Cr-18Mn-0.63N (weight pct) were studied, and the internal stress and effective stress were estimated by partitioning the hysteresis loop during cyclic straining at total strain amplitudes ranging from 3.0 × 10−3 to 1.0 × 10−2. It is found that immediate cyclic softening takes place at all strain amplitudes and subsequently a saturation or quasi-saturation state develops and occupies the main part of the whole fatigue life. The internal stress increases with increasing strain amplitude, while the variation of effective stress with strain amplitude is somewhat complicated. Such a phenomenon is discussed in terms of dislocation structures and the short-range ordering caused by the interaction between nitrogen atoms and substitutional atoms. The relationship of fatigue life vs plastic strain amplitude (Nf−Δεpl/2) follows a bilinear Coffin–Manson rule, resulting from the variation in slip deformation mode with the applied strain amplitude. At the low strain amplitude, cracks initiate along slip bands, and planar slip dislocation configurations dominate the major characteristic of internal microstructures. At high strain amplitudes, intergranular (mostly along grain boundaries and few along twin boundaries) cracks are generally found, and the deformation microstructures are mainly composed of dislocation cells, stacking faults and a small amount of deformation twins, in addition to planar slip dislocation structures.
引用
收藏
页码:1610 / 1620
页数:10
相关论文
共 50 条
  • [31] Kinetics of Cr2N Precipitation and Its Effect on Pitting Corrosion of Nickel-Free High-Nitrogen Austenitic Stainless Steel
    Krishna Kumar, K.
    Anburaj, J.
    Dhanasekar, R.
    Satishkumar, T.
    Abuthakir, J.
    Manikandan, P.
    Subramanian, R.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (09) : 6044 - 6052
  • [32] Nanoindentation creep deformation behaviour of high nitrogen nickel-free austenitic stainless steel
    Zhang, Xiaoru
    Sun, Shicheng
    Sun, Guixun
    Han, Shuang
    Jiang, Zhonghao
    Lian, Jianshe
    MATERIALS SCIENCE AND TECHNOLOGY, 2019, 35 (13) : 1592 - 1599
  • [33] Influence of rare earth Ce on hot deformation behavior of as-cast Mn18Cr18N high nitrogen austenitic stainless steel
    Yushuo Li
    Yanwu Dong
    Zhouhua Jiang
    Qingfei Tang
    Shuyang Du
    Zhiwen Hou
    International Journal of Minerals, Metallurgy and Materials, 2023, 30 : 324 - 334
  • [34] Precipitation of σ-phase in high-nitrogen austenitic 18Cr-18Mn-2Mo-0.9N stainless steel during isothermal aging
    Lee, TH
    Oh, CS
    Lee, CG
    Kim, SJ
    Takaki, S
    SCRIPTA MATERIALIA, 2004, 50 (10) : 1325 - 1328
  • [35] Influence of rare earth Ce on hot deformation behavior of as-cast Mn18Cr18N high nitrogen austenitic stainless steel
    Yushuo Li
    Yanwu Dong
    Zhouhua Jiang
    Qingfei Tang
    Shuyang Du
    Zhiwen Hou
    InternationalJournalofMinerals,MetallurgyandMaterials, 2023, (02) : 324 - 334
  • [36] Corrosion Behavior of High Nitrogen Nickel-Free Fe-16Cr-Mn-Mo-N Stainless Steels
    K. L. Chao
    H. Y. Liao
    J. J. Shyue
    S. S. Lian
    Metallurgical and Materials Transactions B, 2014, 45 : 381 - 391
  • [37] Corrosion Behavior of High Nitrogen Nickel-Free Fe-16Cr-Mn-Mo-N Stainless Steels
    Chao, K. L.
    Liao, H. Y.
    Shyue, J. J.
    Lian, S. S.
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2014, 45 (02): : 381 - 391
  • [38] Influence of rare earth Ce on hot deformation behavior of as-cast Mn18Cr18N high nitrogen austenitic stainless steel
    Li, Yushuo
    Dong, Yanwu
    Jiang, Zhouhua
    Tang, Qingfei
    Du, Shuyang
    Hou, Zhiwen
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2023, 30 (02) : 324 - 334
  • [39] Cavitation Erosion Behaviors of a Nickel-Free High-Nitrogen Stainless Steel
    Yanxin Qiao
    Zhaohui Tian
    Xiang Cai
    Jian Chen
    Yuxin Wang
    Qining Song
    Huabing Li
    Tribology Letters, 2019, 67
  • [40] Cavitation Erosion Behaviors of a Nickel-Free High-Nitrogen Stainless Steel
    Qiao, Yanxin
    Tian, Zhaohui
    Cai, Xiang
    Chen, Jian
    Wang, Yuxin
    Song, Qining
    Li, Huabing
    TRIBOLOGY LETTERS, 2019, 67 (01)