摘要
This report describes an investigation of the hot corrosion resistance of Cr2O3-Al2O3 ceramics in V2O5-Na2SO4 molten salt. Adding Cr2O3 to Al2O3 improves the hot corrosion resistance of Al2O3 ceramics, and thickness of the damage zone depends on the sintering temperature and the Cr2O3 content. Corrosion of the Cr2O3-Al2O3 ceramics is caused by the formation of a liquid of the dissolved Na2O-V2O5-(Al,Cr)2O3 system and by dissolution of the Cr2O3-Al2O3 ceramics into this liquid. The corrosion rate of the Cr2O3-Al2O3 ceramics becomes smaller than that of the Al2O3 ceramics because dissolution rate of grains into the liquid phase occurring in grain boundaries decreases, compared with the Al2O3 ceramics. If the sintering temperature is elevated, grain growth would occur to enhance the corrosion resistance of the ceramics.
引用
收藏
页码:5927 / 5934
页数:7
相关论文
共 50 条
  • [41] FOURIER-TRANSFORM INFRARED SPECTROSCOPIC STUDY OF COKE DEPOSITS ON A CR2O3-AL2O3 CATALYST
    IBARRA, JV
    ROYO, C
    MONZON, A
    SANTAMARIA, J
    VIBRATIONAL SPECTROSCOPY, 1995, 9 (02) : 191 - 196
  • [42] MgO-Al2O3-Cr2O3 refractories of increased corrosion resistance for nonferrous metallurgical furnaces
    Kashcheev, ID
    Semyannikov, VP
    Gel'fenbein, VE
    Bibaev, VM
    Yarushina, TV
    Konygin, VP
    REFRACTORIES AND INDUSTRIAL CERAMICS, 1998, 39 (1-2) : 31 - 35
  • [43] Optimization of corrosion resistance and mechanical properties of Al2O3-Cr2O3 refractories for waste incinerator
    An, Yi
    Liu, Hao
    Wang, Zhoufu
    Ma, Yan
    Wang, Xitang
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2024, 21 (02) : 1104 - 1118
  • [44] MECHANISM OF REACTION OF NITROGEN-OXIDE WITH AMMONIA OVER CR2O3-AL2O3 AND CR2O3 CATALYSTS .1. CHARACTERIZATION OF CATALYSTS
    NIIYAMA, H
    MURATA, K
    EBITANI, A
    ECHIGOYA, E
    JOURNAL OF CATALYSIS, 1977, 48 (1-3) : 194 - 200
  • [45] Corrosion behavior of plasma-sprayed Al2O3-Cr2O3 coatings in hot lithium molten salt
    Cho, Soo Haeng
    Park, Sung Bin
    Kang, Dae Seong
    Jeong, Myeong Soo
    Park, Heong
    Hur, Jin Mok
    Lee, Han Soo
    JOURNAL OF NUCLEAR MATERIALS, 2010, 399 (2-3) : 212 - 218
  • [46] Photoacoustic spectra of mixed ceramics of Al2O3 and Cr2O3
    Toyoda, T
    Yamamoto, H
    Togashi, M
    Shen, Q
    ANALYTICAL SCIENCES, 2001, 17 : S43 - S46
  • [47] Effects of TiO2 addition on phase, mechanical properties, and microstructure of Cr2O3-Al2O3 ceramic composite
    Zhang, Fujun
    Liu, Wei
    Sun, Ye
    Cui, Kunkun
    Yang, Shufeng
    Li, Jingshe
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 2508 - 2527
  • [48] Effect of calcination temperature on the catalytic properties of Cr2O3-Al2O3 aerogels: selective oxidation of toluene to benzaldehyde
    Younes, M. K.
    Ghorbel, A.
    Naccache, C.
    Journal de Chimie Physique et de Physico-Chimie Biologique, 94 (11-12):
  • [49] Effect of calcination temperature on the catalytic properties of Cr2O3-Al2O3 aerogels:: selective oxidation of toluene to benzaldehyde
    Younes, MK
    Ghorbel, A
    Naccache, C
    JOURNAL DE CHIMIE PHYSIQUE ET DE PHYSICO-CHIMIE BIOLOGIQUE, 1997, 94 (11-12) : 1993 - 2006
  • [50] MAGNETIC PROPERTIES OF CHROMIUM IONS IN OXIDE MATRICES .1. CR2O3-AL2O3 SOLID SOLUTIONS
    STONE, FS
    VICKERMAN, JC
    TRANSACTIONS OF THE FARADAY SOCIETY, 1971, 67 (578): : 316 - +