Effect of short-term elevated temperature curing on strength properties and microstructure of fresh fly ash geopolymer mortar

被引:3
|
作者
Uğur Durak
机构
[1] Erciyes University,Civil Engineering Department, Engineering Faculty
关键词
Geopolymer; Fly ash; Alkali-activated mortar; Elevated temperature; Microstructure;
D O I
10.1007/s12517-022-10050-4
中图分类号
学科分类号
摘要
引用
收藏
相关论文
共 50 条
  • [21] Effect of Partial Replacement of Fly Ash by Decoration Waste Powder on the Fresh and Mechanical Properties of Geopolymer Masonry Mortar
    Liu, Hui
    Zhang, Ruidong
    Zhu, Pinghua
    Wang, Xinjie
    Chen, Chunhong
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2024, 39 (03): : 698 - 704
  • [22] Workability and Strength Properties of Class C Fly Ash-Based Geopolymer Mortar
    Cornelis, Remigildus
    Priyosulistyo, Henricus
    Satyarno, Iman
    Rochmadi
    INTERNATIONAL CONFERENCE ON SUSTAINABLE CIVIL ENGINEERING STRUCTURES AND CONSTRUCTION MATERIALS (SCESCM 2018), 2019, 258
  • [23] Effect of nano-silica on strength and durability of fly ash based geopolymer mortar
    Adak, D.
    Sarkar, M.
    Mandal, S.
    CONSTRUCTION AND BUILDING MATERIALS, 2014, 70 : 453 - 459
  • [24] Effect of Elevated Temperature on Mechanical Properties of High-Volume Fly Ash-Based Geopolymer Concrete, Mortar and Paste Cured at Room Temperature
    Zhao, Jun
    Wang, Kang
    Wang, Shuaibin
    Wang, Zike
    Yang, Zhaohui
    Shumuye, Eskinder Desta
    Gong, Xinglong
    POLYMERS, 2021, 13 (09)
  • [25] Effect of Ground Granulated Blast Slag and Temperature Curing on the Strength of Fly Ash-based Geopolymer Concrete
    Kumar, Anil
    Rajkishor
    Kumar, Niraj
    Chhotu, Anil Kumar
    Kumar, Bhushan
    ENGINEERING TECHNOLOGY & APPLIED SCIENCE RESEARCH, 2024, 14 (02) : 13319 - 13323
  • [26] Microstructure and strength development of fly ash-based geopolymer mortar: Role of nano-metakaolin
    Kaur, Mandeep
    Singh, Jaspal
    Kaur, Manpreet
    CONSTRUCTION AND BUILDING MATERIALS, 2018, 190 : 672 - 679
  • [27] INFLUENCE OF WET MILLING OF FLY ASH ON COMPRESSION STRENGTH OF GEOPOLYMER MORTAR CURED AT ROOM TEMPERATURE
    Baheti, Vijay
    Nguyen Thang Xiem
    Militky, Jiri
    Louda, Petr
    STRUTEX: STRUCTURE AND STRUCTURAL MECHANICS OF TEXTILES FABRICS, 2011/STRUKTURNI A STRUKTURNI MECHANIKA TEXTILII, 2011, 2011, : 505 - 511
  • [28] The Effect of Curing Time on The Properties of Fly Ash-based Geopolymer Bricks
    Mastura, W. I. Wan
    Kamarudin, H.
    Nizar, I. Khairul
    Al Bakri, A. M. Mustafa
    Mohammed, H.
    ADVANCED MATERIALS ENGINEERING AND TECHNOLOGY, 2012, 626 : 937 - +
  • [29] The effect of curing on the properties of metakaolin and fly ash-based geopolymer paste
    Gorhan, Gokhan
    Aslaner, Ridvan
    Sinik, Osman
    COMPOSITES PART B-ENGINEERING, 2016, 97 : 329 - 335
  • [30] Effect of elevated temperatures on properties and color intensities of fly ash mortar
    Wang, Her-Yung
    COMPUTERS AND CONCRETE, 2008, 5 (02): : 89 - 100