Investigation of reheat cracking susceptibility in CGHAZ of modified T23 steel

被引:0
|
作者
Ren-yuan Zhou
Shi-xian Li
Li-hui Zhu
Guo-li Zhai
Ming Song
机构
[1] Shanghai University,State Key Laboratory of Advanced Special Steel and Shanghai Key Laboratory of Advanced Ferrometallurgy and School of Materials Science and Engineering
[2] Baoshan Iron & Steel Co.,undefined
[3] Ltd.,undefined
[4] China Special Equipment Inspection and Research Institute,undefined
关键词
Reheat cracking susceptibility; T23 steel; Gleeble-3800 thermal simulator; Precipitate; Ultra-supercritical power plant;
D O I
暂无
中图分类号
学科分类号
摘要
T23 steel (2.25Cr–1Mo–1.6W–0.24V–0.05Nb, in wt.%) has been widely used as water walls in ultra-supercritical (USC) power plants. However, high reheat cracking susceptibility of T23 steel hazarded the safety of USC power plants. It is aimed to improve the reheat cracking susceptibility of T23 steel from the perspective of modifying chemical composition. Gleeble-3800 thermal simulator was used to simulate the coarse-grained heat-affected zone (CGHAZ) in T23 and modified T23 steels via thermal simulation of welding, and then evaluate the reheat cracking susceptibility in CGHAZ of T23 and modified T23 steels by the isothermal slow strain rate tensile test. The microstructure was systematically investigated by optical microscopy, scanning electron microscopy and transmission electron microscopy. The results show that the reheat cracking susceptibility of modified T23 steel is extremely improved. Compared with T23 steel, there are fewer M23C6 particles at the grain boundaries in modified T23 steel, and the degree of intergranular weakening is smaller. At the same time, not only MX in the grain interiors but also the solid-solutioned C and W in the matrix decrease in modified T23 steel, leading to the decline of intragranular strengthening. In addition, small grain size is beneficial to the improvement of the reheat cracking susceptibility of modified T23 steel. The decreased number of M23C6 at grain boundaries helps to retard the formation and propagation of reheat cracks because of decreased denuded zones.
引用
收藏
页码:1417 / 1425
页数:8
相关论文
共 50 条
  • [21] 热处理温度对长期服役T23钢CGHAZ微观组织的影响
    张振华
    尹少华
    孙志强
    焊接, 2023, (10) : 23 - 30
  • [22] Effect of long term high temperature aging on CGHAZ microstructure of T23 water wall welded joint
    Hanjie Xuebao/Transactions of the China Welding Institution, 2024, 45 (01): : 109 - 115
  • [23] Evaluation of reheat cracking susceptibility of 780 MPa high strength steel welds with low cold cracking sensitivity
    Nakamura, M
    Horie, H
    Tomida, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1998, 84 (10): : 755 - 761
  • [24] The causes of low impact strength of T23 steel weld joints
    Adamiec, Janusz
    Pikos, Izabela
    Stopyra, Michal
    Solid State Phenomena, 2015, 226 : 103 - 106
  • [25] Effect of oxidation on the creep rupture life of ASME T23 steel
    Sawada, Kota
    Fujitsuka, Masakazu
    Tabuchi, Masaaki
    Kimura, Kazuhiro
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2009, 86 (10) : 693 - 698
  • [26] Stress-relief cracking mechanism in simulated coarse-grained heat-affected zone of T23 steel
    Li, Yong
    Wang, Xue
    Wang, Jiaqing
    Chen, Ansheng
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2019, 266 : 73 - 81
  • [27] Effect of Carbon on Stress-Relief Cracking Susceptibility of T23 Steel A new viewpoint was put forward that the precipitation of M23C6 at the grain boundary is the main reason for SRC
    Wang, X.
    Zhang, D.
    Li, Y.
    Lai, X.
    Zhang, W.
    WELDING JOURNAL, 2022, 101 (10) : 253S - 268S
  • [28] Influence of Boron on Stress-Relief Cracking Susceptibility of T23 Steel The effects of increasing boron content levels in the coarse grain heat-affected zone are analyzed
    Zhang, D.
    Wang, X.
    WELDING JOURNAL, 2024, 103 (01) : 1S - 11S
  • [29] Influence of carbon and boron on reheat cracking susceptibility in weld metal of Cr-Mo steel
    Masao Y.
    Kenji H.
    1600, Japan Welding Society (35): : 122 - 128
  • [30] A comparison of the reheat cracking susceptibility of a service exposed high temperature alloy steel with that of new material
    Loots, R
    van Rooyen, GT
    JOURNAL OF THE SOUTH AFRICAN INSTITUTE OF MINING AND METALLURGY, 2004, 104 (11): : 627 - 631