Steam Oxidation Behavior of Advanced Steels and Ni-Based Alloys at 800 °C

被引:0
|
作者
T. Dudziak
L. Boroń
V. Deodeshmukh
J. Sobczak
N. Sobczak
M. Witkowska
W. Ratuszek
K. Chruściel
机构
[1] Foundry Research Institute,Faculty of Metals Engineering and Industrial Computer Science
[2] Haynes International,undefined
[3] AGH University Science and Technology,undefined
关键词
advanced steels; Haynes; internal oxidation; steam oxidation;
D O I
暂无
中图分类号
学科分类号
摘要
This publication studies the steam oxidation behavior of advanced steels (309S, 310S and HR3C) and Ni-based alloys (Haynes® 230®, alloy 263, alloy 617 and Haynes® 282®) exposed at 800 °C for 2000 h under 1 bar pressure, in a pure water steam system. The results revealed that all exposed materials showed relatively low weight gain, with no spallation of the oxide scale within the 2000 h of exposure. XRD analysis showed that Ni-based alloys developed an oxide scale consisting of four main phases: Cr2O3 (alloy 617, Haynes® 282®, alloy 263 and Haynes® 230®), MnCr2O4 (alloy 617, Haynes® 282® and Haynes® 230®), NiCr2O4 (alloy 617) and TiO2 (alloy 263, Haynes® 282®). In contrast, advanced steels showed the development of Cr2O3, MnCr2O4, Mn7SiO12, FeMn(SiO4) and SiO2 phases. The steel with the highest Cr content showed the formation of Fe3O4 and the thickest oxide scale.
引用
收藏
页码:1044 / 1056
页数:12
相关论文
共 50 条
  • [31] Oxidation Behavior of Ni-3,6, 10 wt.% Al Alloys at 800°C
    Shigenari Hayashi
    Saori Narita
    Toshio Narita
    Oxidation of Metals, 2006, 66 : 191 - 207
  • [32] Steam Effects on the Oxidation Behaviour of Al2O3-Scale Forming Ni-Based Alloys
    Wei Zhao
    Brian Gleeson
    Oxidation of Metals, 2013, 79 : 613 - 625
  • [33] Steam Effects on the Oxidation Behaviour of Al2O3-Scale Forming Ni-Based Alloys
    Zhao, Wei
    Gleeson, Brian
    OXIDATION OF METALS, 2013, 79 (5-6): : 613 - 625
  • [34] Oxidation behavior of Ni-3,6, 10 wt.% al alloys at 800°C
    Hayashi, Shigenari
    Narita, Saori
    Narita, Toshio
    OXIDATION OF METALS, 2006, 66 (3-4): : 191 - 207
  • [35] Early stage oxidation behavior of Al- and Si-alloyed stainless steels as well as Ni-based alloys in air at elevated temperatures
    Romu, Jyrki
    Sarikka, Teemu
    Heikkila, Mikko
    Virkkunen, Iikka
    Hanninen, Hannu
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2018, 69 (06): : 690 - 702
  • [36] Oxide Growth Behaviour of 800H and HR-120 Series Ni-based Alloys on Isothermal Oxidation
    Zainal, Nurul Athirah
    Parimin, Noraziana
    Anuar, Aqmar Ikhmal
    Hayazi, Nur Farhana
    Zainal, Farah Farhana
    INTERNATIONAL JOURNAL OF NANOELECTRONICS AND MATERIALS, 2024, 17 (03): : 416 - 421
  • [37] Oxidation ahead of a crack tip in an advanced Ni-based superalloy
    Kitaguchi, H. S.
    Li, H. Y.
    Evans, H. E.
    Ding, R. G.
    Jones, I. P.
    Baxter, G.
    Bowen, P.
    ACTA MATERIALIA, 2013, 61 (06) : 1968 - 1981
  • [38] Oxidation behavior of GTD111 Ni-based superalloy at 900 °C in air
    Brenneman, J.
    Wei, J.
    Sun, Z.
    Liu, L.
    Zou, G.
    Zhou, Y.
    CORROSION SCIENCE, 2015, 100 : 267 - 274
  • [39] Influence of Micro-structure on Oxidation behavior of a Ni-based superalloy at 1000°C
    Liu, Li
    Li, Ying
    Wang, Fuhui
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 7, PTS 1 AND 2, 2008, 595-598 : 87 - 94
  • [40] The Isothermal Oxidation of a New Polycrystalline Turbine Disk Ni-Based Superalloy at 800 °C and Its Modification with Pre-oxidation
    J. W. X. Wo
    H. T. Pang
    A. S. Wilson
    M. C. Hardy
    H. J. Stone
    Metallurgical and Materials Transactions A, 2023, 54 : 1946 - 1960