Low-temperature plasma-enhanced atomic layer deposition growth of WNxCy from a novel precursor for barrier applications in nanoscale devices
被引:0
|作者:
Zeng W.
[1
]
Wang X.
[1
]
Kumar S.
[1
]
Peters D.W.
[2
]
Eisenbraun E.T.
[1
]
机构:
[1] College of Nanoscale Science and Engineering, University of Albany, Albany
[2] Praxair Inc., Tonawanda
来源:
关键词:
Annealing - Atomic layer deposition - Copper - Crystal structure - Electric conductivity - Plasma applications - Surface roughness - Thermodynamic stability - Tungsten compounds;
D O I:
10.1557/jmr.2007.0079
中图分类号:
学科分类号:
摘要:
A low-temperature plasma-enhanced atomic layer deposition (PEALD) process has been developed for the growth of ultrathin WNxCy films, using a halide-free W precursor. A 32-nm-thick PEALD WNxCy film deposited using this process at 250 °C possesses a composition of W72C20N5, resistivity of ∼25 μΩ·cm, a root-mean-square (rms) surface roughness of 0.23 nm, and a thickness conformality of more than 80% on trench structures with a width of 120 nm and an aspect ratio of 11. The WNxCy films exhibited excellent thermal stability, whereby resistivity, thickness, surface roughness, and crystal structure were stable after 30 min anneals in 700 Torr, forming gas ambient at temperatures up to 700 °C. Copper diffusion barrier performance measurements show that a 9 nm thick WNxCy film could prevent copper diffusion after a 30 min anneal at 700 °C, while a 2-nm-thick film could prevent copper diffusion after a 30 min anneal at 500 °C. © 2007 Materials Research Society.