Influence of welding speed on the root defects formation and mechanical properties of FSWed 6082-T6 Al alloy joint

被引:0
|
作者
Qilei Dai
Lei Jin
Kairen Meng
Huijie Liu
Qingyu Shi
Gaoqiang Chen
机构
[1] Tsinghua University,Department of Mechanical Engineering
[2] Hwaway Technology Co.,State Key Laboratory of Advanced Welding and Joining
[3] Ltd.,undefined
[4] Harbin Institute of Technology,undefined
关键词
Friction stir welding; Aluminum alloys; Root defect; Microstructure and property; Kissing bond;
D O I
暂无
中图分类号
学科分类号
摘要
In this paper, 5-mm thick 6082-T6 aluminum alloy plates were friction stir welded in a position control mode at rotation rate of 1800 rpm and welding speeds ranging from 200 to 600 mm/min. The metallurgical morphology of root defects was elucidated. As indicated by observation on electropolished samples that contains the root defects, it was found that there are three types of bonding states near the faying surface at the joint root, which are fully bonded state without cracks, incomplete bonding state in the form of non-continuous cracks (the kissing bond), and unbonded state in the form of continuous cracks (the lack-of-penetration defect). The vertical position of welding tool during the welding pocess is recorded, and it is found that, as the welding speed increased, the rebound amount of the welding tool increased during actual welding process because of increasing deformation resistance. It consequently leads to the decrease of insertion depth of the welding tool, which significantly increases formation tendency of the root defect.
引用
收藏
页码:1097 / 1106
页数:9
相关论文
共 50 条
  • [31] Microstructure and Mechanical Properties of Thick Plate Friction Stir Welds for 6082-T6 Aluminum Alloy
    Liang, Zhimin
    Wang, Xue
    Cai, Congwei
    Wang, Dianlong
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2019, 38 (2019) : 525 - 532
  • [32] Laser Welding of 6082-T6 Al Alloy and 301L Stainless Steel in a Butt Joint Configuration with a High-entropy Alloy (HEA) Interlayer
    Hou, H. Z.
    Gu, X. P.
    Xu, G. C.
    Gu, X. Y.
    Dong, J.
    LASERS IN ENGINEERING, 2023, 54 (1-3) : 157 - 167
  • [33] Microstructure and fatigue damage mechanism of 6082-T6 aluminium alloy welded joint
    Zhu, Minqi
    Yang, Shanglei
    Bai, Yishan
    Fan, Cong
    MATERIALS RESEARCH EXPRESS, 2021, 8 (05)
  • [34] Laser Welding of 6082-T6 Al Alloy and 301L Stainless Steel in a Butt Joint Configuration with a High-entropy Alloy (HEA) Interlayer
    Zhou, H.
    Gu, X.P.
    Xu, G.C.
    Gu, X.Y.
    Dong, J.
    Lasers in Engineering, 2023, 54 (1-3): : 157 - 167
  • [35] Corrosion behavior of 6082-T6 Al joint welded with Twin Wire MIG
    Ruan, Ye
    Qiu, Xiao Ming
    Gong, Wen Biao
    MATERIALS PROCESSING TECHNOLOGY, PTS 1-3, 2012, 418-420 : 1368 - +
  • [36] Experimental and numerical study to minimize the residual stresses in welding of 6082-T6 aluminum alloy
    Costa, Sharlane
    Souza, Maria S.
    Cesar, Manuel B.
    Goncalves, Jose
    Ribeiro, Joao E.
    AIMS MATERIALS SCIENCE, 2021, 8 (02) : 271 - 282
  • [37] Experimental comparison of friction stir welding process and TIG welding process for 6082-T6 Aluminium alloy
    Singh, Gurmeet
    Kang, Amardeep S.
    Singh, Kulwant
    Singh, Jagtar
    MATERIALS TODAY-PROCEEDINGS, 2017, 4 (02) : 3590 - 3600
  • [39] Mechanical properties and microstructures of 6082-T6 joint welded by twin wire metal inert gas arc welding with the SiO2 flux
    Ruan, Y.
    Qiu, X. M.
    Gong, W. B.
    Sun, D. Q.
    Li, Y. P.
    MATERIALS & DESIGN, 2012, 35 : 20 - 24
  • [40] Metallurgical and Mechanical Characterization of High-Speed Friction Stir Welded AA 6082-T6 Aluminum Alloy
    Naumov, Anton
    Morozova, Iuliia
    Rylkov, Evgenii
    Obrosov, Aleksei
    Isupov, Fedor
    Michailov, Vesselin
    Rudskoy, Andrey
    MATERIALS, 2019, 12 (24)