摘要
The catalytic wet oxidation process is the most attractive process for small-scale hydrogen sulfide (H2S) removal from natural gas. The catalytic wet oxidation process is anticipated to be cost effective and simple so that it can be used for treating sour gases containing small amounts of H2S and can be easily operated even in isolated sites. The development of effective catalyst is the key technology in the wet catalytic oxidation of H2S. The scale of operation for the process has to be flexible so its use will not be limited by the flow rates of the gas to be treated. The heterogeneous catalytic wet oxidation of H2S has been attempted on activated carbons, but the H2S removal capacity still shows the low removal efficiency. The catalytic wet oxidation of H2S was studied over Fe/MgO for an effective removal of H2S. In order to develop a sulfur removal technology, one has to know what surface species of catalyst are the most active. This article discusses the following systematic studies: (i) the catalytic preparation to disperse Fe metal well on MgO support for enhancing H2S removal capacity, (ii) the effect of the catalytic morphology on the activity of Fe/MgO for the H2S wet oxidation, (iii) the influence of precursor and support on the activity of Fe/MgO for catalytic wet oxidation of H2S to sulfur.
引用
收藏
页码:134 / 144
页数:10
相关论文
共 50 条
  • [41] Low temperature catalytic oxidation of H2S over V2O5/CeO2 catalysts
    Palma, V.
    Barba, D.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2014, 39 (36) : 21524 - 21530
  • [42] Patented wet H2S cracking inhibitor
    不详
    HYDROCARBON PROCESSING, 1999, 78 (04): : 35 - 36
  • [43] WET SCRUBBER SOLVES H2S ODORS
    不详
    POLLUTION ENGINEERING, 1995, 27 (05) : 61 - 61
  • [44] CATALYTIC REACTION OF TETRAHYDROFURAN WITH H2S
    DESYATOV, IV
    YAKOVLEVA, VN
    MASHKINA, AV
    REACTION KINETICS AND CATALYSIS LETTERS, 1990, 41 (01): : 97 - 102
  • [45] Two-dimensional CaO/carbon heterostructures with unprecedented catalytic performance in room-temperature H2S oxidization
    Pan, Yankai
    Chen, Mingqi
    Su, Zhe
    Wu, Kede
    Zhang, Yayun
    Long, Donghui
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2021, 280
  • [46] Role of Pore Structure of Activated Carbon Fibers in the Catalytic Oxidation of H2S
    Chen, Qingjun
    Wang, Zhi
    Long, Donghui
    Liu, Xiaojun
    Zhan, Liang
    Liang, Xiaoyi
    Qiao, Wenming
    Ling, Licheng
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2010, 49 (07) : 3152 - 3159
  • [47] Hydrothermally synthesized CeO2 nanowires for H2S sensing at room temperature
    Li, Zhijie
    Niu, Xinyue
    Lin, Zhijie
    Wang, Ningning
    Shen, Huahai
    Liu, Wei
    Sun, Kai
    Fu, Yong Qing
    Wang, Zhiguo
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 682 : 647 - 653
  • [48] CdS thin film sensor for NO2 and H2S detection at room temperature
    Perillo, P. M.
    Rodriguez, D. F.
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2024, 130 (06):
  • [49] Study on the essential features for MOFs to reversible adsorption of H2S at room temperature
    Yang, Yongjie
    Liu, Xuan
    Yang, Chao
    Wang, Yeshuang
    Wang, Hui
    Fan, Huiling
    COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2023, 674
  • [50] Reactivity of a FeS Surface under Room Temperature Exposure to Nitrogen and H2S
    Nino, Miguel A.
    Flores, Eduardo
    Sanchez, Carlos
    Rojo, Juan M.
    JOURNAL OF PHYSICAL CHEMISTRY B, 2018, 122 (02): : 705 - 712