Type II Hot Corrosion Screening Tests of a Cr2AlC MAX Phase Compound

被引:0
|
作者
James L. Smialek
Simon Gray
机构
[1] NASA Glenn Research Center,
[2] Cranfield University,undefined
来源
Oxidation of Metals | 2018年 / 90卷
关键词
Cr; AlC MAX phase; Hot corrosion; Superalloys;
D O I
暂无
中图分类号
学科分类号
摘要
Low-temperature hot corrosion tests were performed on bulk Cr2AlC MAX phase compounds for the first time. This material is a known alumina-former with good oxidation and Type I high-temperature hot corrosion resistance. Unlike traditional (Ni,Co)CrAl alumina formers, it contains no Ni or Co that may react with Na2SO4 salt deposits needed to form corrosive mixed (Ni,Co)SO4–Na2SO4 eutectic salts active in Type II hot corrosion. Cr2AlC samples coated with 20K2SO4–80Na2SO4 salt were exposed to 300 ppm SO2 at 700 °C for times up to 500 h. Weight change, recession, and cross-sectional microstructures identified some reactivity, but much reduced (< 1/10) compared to a Ni(Co) superalloy baseline material. Layered Al2O3/Cr2O3 scales were indicated, either separated by or intermixed with some retained salt. However, there was no conclusive indication of salt melting. Accelerated oxidation was proposed to explain the results, and coarse Cr7C3 impurities appeared to play a negative role. In contrast, the superalloy exhibited outer Ni(Co) oxide and inner Cr2O3 scales, with Cr–S layers at the interfaces. Massive spallation of the corrosion layers occurred repeatedly for the superalloy, but not at all for Cr2AlC. This indicates some potential for Cr2AlC as LTHC-resistant coatings for superalloys.
引用
收藏
页码:555 / 570
页数:15
相关论文
共 50 条
  • [31] Electrochemical Corrosion Inhibition of Cr2AlC MAX Phase Coatings via Mo Solid Solution: Comprehensive Experimental and Simulation Study
    Zhang, Yan
    Zhang, Anfeng
    Li, Zhongchang
    Wang, Zhenyu
    Ke, Peiling
    Wang, Aiying
    JOURNAL OF PHYSICAL CHEMISTRY C, 2024, 128 (09): : 3916 - 3923
  • [32] Nanostructured plasma etched, magnetron sputtered nanolaminar Cr2AlC MAX phase thin films
    Grieseler, Rolf
    Haehnlein, Bernd
    Stubenrauch, Mike
    Kups, Thomas
    Wilke, Marcus
    Hopfeld, Marcus
    Pezoldt, Joerg
    Schaaf, Peter
    APPLIED SURFACE SCIENCE, 2014, 292 : 997 - 1001
  • [33] Processing and oxidation response of Cr2AlC MAX-phase composites containing ceramic fibers
    Go, Teresa
    Vassen, Robert
    Guillon, Olivier
    Gonzalez-Julian, Jesus
    OPEN CERAMICS, 2021, 6
  • [34] Mechanical properties of SPS-processed Cr2AlC MAX phase with different impurity contents
    Shamsipoor, A.
    Farvizi, M.
    Mousavi, B.
    EMERGENT MATERIALS, 2023, 6 (03) : 965 - 972
  • [35] Exploring the potential application of Cr2AlC MAX phase as an emerging electrocatalyst for overall water splitting
    Ramachandra, Madhushree
    Pai, Sunaja Devi Kalathiparambil Rajendra
    EMERGENT MATERIALS, 2024,
  • [36] Crack healing behaviour of Cr2AlC MAX phase studied by X-ray tomography
    Pei, R.
    McDonald, S. A.
    Shen, L.
    van der Zwaag, S.
    Sloof, W. G.
    Withers, P. J.
    Mummery, P. M.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (02) : 441 - 450
  • [37] High-temperature synthesis of a cast material with a maximum content of the MAX phase Cr2AlC
    Gorshkov, V. A.
    Miloserdov, P. A.
    Luginina, M. A.
    Sachkova, N. V.
    Belikova, A. F.
    INORGANIC MATERIALS, 2017, 53 (03) : 271 - 277
  • [38] Cold spray deposition of Cr2AlC MAX phase for coatings and bond-coat layers
    Go, T.
    Sohn, Y. J.
    Mauer, G.
    Vassen, R.
    Gonzalez-Julian, J.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (04) : 860 - 867
  • [39] Comparison of the High-Temperature Oxidation Behavior of Cr2AlC MAX Phase and CoNiCrAlY Compounds
    Shamsipoor, A.
    Farvizi, M.
    Razavi, M.
    Keyvani, A.
    Mousavi, B.
    OXIDATION OF METALS, 2021, 95 (1-2): : 1 - 21
  • [40] High-temperature synthesis of a cast material with a maximum content of the MAX phase Cr2AlC
    V. A. Gorshkov
    P. A. Miloserdov
    M. A. Luginina
    N. V. Sachkova
    A. F. Belikova
    Inorganic Materials, 2017, 53 : 271 - 277