Effect of Chemical Composition and Structure on Mechanical Properties of High-Strength Welding Steels

被引:0
|
作者
V. M. Goritskii
G. R. Shneiderov
I. A. Guseva
机构
[1] CJSC “Melnikov Central Research and Design Institute of Steel Structures”,
来源
Metallurgist | 2019年 / 63卷
关键词
thermomechanical rolling; high-strength steel; mechanical properties; impact toughness; impact toughness anisotropy factor; steel structure;
D O I
暂无
中图分类号
学科分类号
摘要
Based on the analysis of the Russian-made 4 to 16 mm thick rolled products produced by thermomechanical rolling from high-strength (yield point: 433 to 828 MPa) low-alloyed welding steels obtained as a result of 15 melting runs, the effect of chemical composition and structure on the mechanical properties, such as yield point, impact toughness, and impact toughness anisotropy factor, was studied. It was shown that the yield point of manganese steel (1.62–1.80 wt. % Mn) is mainly caused by microalloying with titanium, and to a lesser degree – with niobium and vanadium. An increase in the yield point of steel in excess of 700 MPa increases its tendency to impact toughness anisotropy. Within the concentration range from 0.001 to 0.08 wt. % Ti, the value of anisotropy factor Ka , which varies from 1.45 to 1.80, does not depend on Ti content, but increases sharply to Ka = 3.19 once the Ti content increases (in excess of 0.08 wt. %). A considerable negative effect of Nb content in steel on impact toughness (KCV– 40), measured on transverse specimens, has been established. A joint negative effect of Ti + Al on KCV– 40 is somewhat less pronounced. The presence of Al in the inclusions of complex composition (Ti-Al-Cr) noticeably reduces (by 4.5 times) the negative effect of Ti on KCV– 40 of highstrength manganese steel.
引用
收藏
页码:21 / 32
页数:11
相关论文
共 50 条
  • [11] MECHANICAL PROPERTIES AND FRACTURE BEHAVIOR OF HIGH-STRENGTH STEELS
    Musalek, R.
    Hausild, P.
    Siegl, J.
    Bensch, J.
    Slama, J.
    STRENGTH OF MATERIALS, 2008, 40 (01) : 142 - 145
  • [12] Mechanical properties and fracture behavior of high-strength steels
    R. Mušálek
    P. Haušild
    J. Siegl
    J. Bensch
    J. Sláma
    Strength of Materials, 2008, 40 : 142 - 145
  • [13] Effect of heat treatment on mechanical properties and structure of high-strength pipe steels with a ferrite-bainite structure
    M. Yu. Matrosov
    O. P. Talanov
    I. V. Lyasotskii
    D. L. Dyakonov
    E. I. Khlusova
    V. V. Orlov
    A. M. Korchagin
    D. S. Tsvetkov
    S. D. Popova
    Metallurgist, 2011, 55 : 489 - 495
  • [14] EFFECT OF HEAT TREATMENT ON MECHANICAL PROPERTIES AND STRUCTURE OF HIGH-STRENGTH PIPE STEELS WITH A FERRITE-BAINITE STRUCTURE
    Matrosov, M. Yu
    Talanov, O. P.
    Lyasotskii, I. V.
    Dyakonov, D. L.
    Khlusova, E. I.
    Orlov, V. V.
    Korchagin, A. M.
    Tsvetkov, D. S.
    Popova, S. D.
    METALLURGIST, 2011, 55 (7-8) : 582 - 590
  • [15] Laser Blank Welding High-Strength Steels
    Haiping Shao
    Jerry Gould
    Charlie Albright
    Metallurgical and Materials Transactions B, 2007, 38 : 321 - 331
  • [16] WELDING COMMON CONSTRUCTIONAL HIGH-STRENGTH STEELS
    BAXTER, DF
    METAL PROGRESS, 1971, 99 (05): : 82 - &
  • [17] LATEST DEVELOPMENTS IN WELDING OF HIGH-STRENGTH STEELS
    BAKER, RG
    JOURNAL OF THE AUSTRALASIAN INSTITUTE OF METALS, 1968, 13 (03): : 149 - &
  • [18] WELDING OF MODERN HIGH-STRENGTH CONSTRUCTION STEELS
    UWER, D
    DEGENKOLBE, J
    HERR, D
    STAHL UND EISEN, 1991, 111 (11): : I36 - I36
  • [19] FORMING AND WELDING HIGH-STRENGTH SHEET STEELS
    VACCARI, JA
    AMERICAN MACHINIST, 1984, 128 (05) : 109 - 124
  • [20] Laser blank welding high-strength steels
    Shao, Haiping
    Gould, Jerry
    Albright, Charlie
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2007, 38 (02): : 321 - 331