Oxidation Behavior of Ni3Al and Fe3Al: II. Early Stage of Oxide Growth

被引:0
|
作者
A. Velon
I. Olefjord
机构
[1] Chalmers University of Technology,Department of Engineering Metals
来源
Oxidation of Metals | 2001年 / 56卷
关键词
Ni; Al; Fe; Al; oxidation mechanisms; air; XPS; AES;
D O I
暂无
中图分类号
学科分类号
摘要
Oxidation treatments of Ni3Al and Fe3Al were performed at room temperature in 0.2 atm O2 for 5 min and at 300 and 500°C in air for 5 min, and 6, 50, 100, and 200 hr. The oxides were analyzed by XPS, AES, and SEM. A model explaining the initial stages of oxide formation is suggested. At room temperature and 300°C, islands of Al2O3 and NiO combined with NiAl2O4 formed on Ni3Al. At 500°C, the Ni oxides grow laterally and cover the Al2O3 islands. Islands of Al2O3 and Fe2O3 mixed with Fe(Fe, Al)2O4 formed on Fe3Al at room temperature. At 300 and 500°C the scale is composed of an outer layer rich in Fe oxides and an inner layer rich in Al oxides. During long time exposure, islands of Fe2O3 and Fe(Fe, Al)2O4 formed at the surface by diffusion of Fe cations through the alumina layer. The oxide growth on Fe3Al reaches a steady-state regime after formation of the continuous alumina layer. At 300°C, the oxide formed on Fe3Al is thicker than on Ni3Al, whereas it is reverse at 500°C.
引用
收藏
页码:425 / 452
页数:27
相关论文
共 50 条
  • [21] Structural heat-resistant β-NiAl + γ′-Ni3Al alloys of the Ni–Al–Co system: II. Oxidation
    Povarova K.B.
    Drozdov A.A.
    Bazyleva O.A.
    Morozov A.E.
    Antonova A.V.
    Arginbaeva E.G.
    Alad’ev N.A.
    Sirotinkin V.P.
    Russian Metallurgy (Metally), 2017, 2017 (9) : 706 - 710
  • [22] Oxidation and sulfidation of Ni3Al
    Lee, WH
    MATERIALS CHEMISTRY AND PHYSICS, 2002, 76 (01) : 26 - 37
  • [23] Effect of yttrium coating on the oxidation behavior of Ni3Al
    Jung, HG
    Kim, KY
    OXIDATION OF METALS, 1996, 46 (1-2): : 147 - 167
  • [24] Effect of Ce on oxidation behavior of Ni3Al alloys
    Xi, T.H.
    Yuan, Z.X.
    Yu, Z.S.
    Acta Metallurgica Sinica Series A, Physical Metallurgy & Materials Science, 1997, 10 (01): : 74 - 78
  • [25] EARLY STAGE OF NI3AL LAYER GROWTH IN NIAL/NI DIFFUSION COUPLES.
    GLITZ, R.
    NOTIS, M.R.
    GOLDSTEIN, J.I.
    1982, V 13A (N 11): : 1921 - 1926
  • [26] Magnetism of Ni3Al and Fe3Al under extreme pressure and shape deformation:: an ab initio study
    Sob, M.
    Legut, D.
    Friak, M.
    Fiala, J.
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2004, 272 : E205 - E206
  • [27] High-Temperature Oxidation Behavior of ODS–Fe3Al
    I. G. Wright
    B. A. Pint
    P. F. Tortorelli
    Oxidation of Metals, 2001, 55 : 333 - 357
  • [28] Oxidation kinetics of microcrystalline Ni3Al
    Wang, YG
    Ma, TJ
    He, YD
    Zhu, RZ
    Zheng, XL
    RARE METAL MATERIALS AND ENGINEERING, 1998, 27 (03) : 149 - 151
  • [29] Oxidation Kinetics of Macrocrystalline Ni3Al
    Wang, Yonggang
    Ma, Tiejun
    He, Yedong
    Zhu, Rizhang
    Zheng, Xiulin
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 1998, 27 (03):
  • [30] High-temperature oxidation behavior of pure Ni3Al
    Choi, SC
    Cho, HJ
    Kim, YJ
    Lee, DB
    OXIDATION OF METALS, 1996, 46 (1-2): : 51 - 72