Oxidation treatments of Ni3Al and Fe3Al were performed at room temperature in 0.2 atm O2 for 5 min and at 300 and 500°C in air for 5 min, and 6, 50, 100, and 200 hr. The oxides were analyzed by XPS, AES, and SEM. A model explaining the initial stages of oxide formation is suggested. At room temperature and 300°C, islands of Al2O3 and NiO combined with NiAl2O4 formed on Ni3Al. At 500°C, the Ni oxides grow laterally and cover the Al2O3 islands. Islands of Al2O3 and Fe2O3 mixed with Fe(Fe, Al)2O4 formed on Fe3Al at room temperature. At 300 and 500°C the scale is composed of an outer layer rich in Fe oxides and an inner layer rich in Al oxides. During long time exposure, islands of Fe2O3 and Fe(Fe, Al)2O4 formed at the surface by diffusion of Fe cations through the alumina layer. The oxide growth on Fe3Al reaches a steady-state regime after formation of the continuous alumina layer. At 300°C, the oxide formed on Fe3Al is thicker than on Ni3Al, whereas it is reverse at 500°C.
引用
收藏
页码:425 / 452
页数:27
相关论文
共 50 条
  • [1] Oxidation behavior of Ni3Al and Fe3Al:: II.: Early stage of oxide growth
    Velon, A
    Olefjord, I
    OXIDATION OF METALS, 2001, 56 (5-6): : 425 - 452
  • [2] Influence of Cr on the oxidation of Fe3Al and Ni3Al at 500°C
    Velon, A
    Yi, DQ
    OXIDATION OF METALS, 2002, 57 (1-2): : 13 - 31
  • [3] Influence of Cr on the Oxidation of Fe3Al and Ni3Al at 500°C
    A. Velon
    D.-Q. Yi
    Oxidation of Metals, 2002, 57 : 13 - 31
  • [4] An overview of the welding of Ni3Al and Fe3Al alloys
    Santella, ML
    INTERNATIONAL SYMPOSIUM ON NICKEL AND IRON ALUMINIDES: PROCESSING, PROPERTIES, AND APPLICATIONS, 1997, : 321 - 327
  • [5] Oxidation Behavior of Ni3Al and Fe3Al: I. XPS Calibrations of Pure Compounds and Quantification of the Results
    A. Velon
    I. Olefjord
    Oxidation of Metals, 2001, 56 : 415 - 424
  • [6] Oxidation behavior of Ni3Al and Fe3Al:: I.: XPS calibrations of pure compounds and quantification of the results
    Velon, A
    Olefjord, I
    OXIDATION OF METALS, 2001, 56 (5-6): : 415 - 424
  • [7] Intermetallids Ni3Al and Fe3Al with directional structure as future materials
    Verin, AS
    Verin, MA
    ANTI-CORROSION METHODS AND MATERIALS, 2001, 48 (05) : 298 - 303
  • [8] Effect of a yttrium coating on the oxidation behavior of Ni3Al (II)
    Jung, HG
    Kim, KY
    OXIDATION OF METALS, 1998, 49 (5-6): : 403 - 430
  • [9] Effect of a Yttrium Coating on the Oxidation Behavior of Ni3Al (II)
    Hwan Gyo Jung
    Kyoo Young Kim
    Oxidation of Metals, 1998, 49 : 403 - 430
  • [10] Metal dusting of Fe3Al and (Fe,Ni)(3)Al
    Strauss, S
    Krajak, R
    Palm, M
    Grabke, HJ
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1996, 47 (12): : 701 - 702