Durability of plasma-sprayed Cr3C2-NiCr coatings under rolling contact conditions

被引:5
|
作者
Zhang X. [1 ,2 ]
Xuan F. [1 ]
Tu S. [1 ]
Xu B. [2 ]
Wu Y. [2 ]
机构
[1] Key Laboratory of Safety Science of Pressurized System, Ministry of Education, East China University of Science and Technology
[2] Shanghai Key Lab of Materials Laser Processing and Modification, Shanghai Jiao Tong University
基金
中国国家自然科学基金;
关键词
coating; failure mode; mechanism; rolling contact fatigue; Weibull distribution;
D O I
10.1007/s11465-011-0127-0
中图分类号
学科分类号
摘要
The aim of this paper was to address the rolling contact fatigue (RCF) failure mechanisms of plasmasprayed Cr3C2-NiCr coatings under different tribological conditions of contact stress. Weibull distribution plots of fatigue lives of the coated specimens at different contact stresses were obtained. The failure modes of coatings were identified on the basis of wore surface observations of the failed coatings. Results showed that the RCF failure modes can be classified into four main categories, i. e., surface abrasion, spalling, cohesive delamination, and interfacial delamination. The probabilities of the surface abrasion and spalling type failures were relatively high at low contact stress. When the coatings were subjected to abrasion and spalling type failures, the failure of the coating was depended on the microstrcture of the coating. The stress concentration near the micro-defects in the coating may be the may reason for the formation of spall. The coatings were prone to fail in delamination under higher contact stresses. However, the delamination of coating may be related to distribution of shear stress amplitude within coating. The location of maximum shear stress amplitude can be used as a key parameter to predict the initiation of subsurface cracks within coating in rolling contact. © 2011 Higher Education Press and Springer-Verlag Berlin Heidelberg.
引用
收藏
页码:118 / 135
页数:17
相关论文
共 50 条
  • [42] Erosion and corrosion behavior of shrouded plasma sprayed Cr3C2-NiCr coating
    Lu, Haiyang
    Shang, Jiantong
    Jia, Xiujie
    Li, Yanle
    Li, Fangyi
    Li, Jianfeng
    Nie, Yanyan
    SURFACE & COATINGS TECHNOLOGY, 2020, 388
  • [44] Erosion Behaviour of Thermal Sprayed Cr3C2-NiCr Coatings at Room and Elevated Temperatures
    Vicenzi, Juliane
    Marques, Caio Marcelo
    Bergmann, Carlos Perez
    SOLDAGEM & INSPECAO, 2008, 13 (03): : 219 - 226
  • [45] Solid Particle Erosion Behaviour of Plasma-Sprayed (WC–Co)/(Cr3C2–NiCr) Coatings
    Reddy G.M.S.
    Ramesh S.
    Anne G.
    Ramesh M.R.
    Rao T.N.
    Patil P.
    Journal of Bio- and Tribo-Corrosion, 2022, 8 (02)
  • [46] Fractal character of circumferences of polishing-induced pull outs of plasma sprayed Cr3C2-NiCr coatings
    Li, JF
    Ding, CX
    THIN SOLID FILMS, 2000, 376 (1-2) : 179 - 182
  • [47] Fatigue resistance and failure mechanisms of plasma-sprayed CrC-NiCr cermet coatings in rolling contact
    Zhang, X. C.
    Xu, B. S.
    Tu, S. T.
    Xuan, F. Z.
    Wang, H. D.
    Wu, Y. X.
    INTERNATIONAL JOURNAL OF FATIGUE, 2009, 31 (05) : 906 - 915
  • [48] Comparison of Four Different Methods to Determine the Hardness of Plasma-sprayed Cr3C2-NiCr Coating by Nano-indentation
    Zhu, Li-na
    Xu, Bin-shi
    Wang, Hai-dou
    Wang, Cheng-biao
    JOURNAL OF TESTING AND EVALUATION, 2015, 43 (01) : 108 - 114
  • [49] Cracking resistance of Cr3C2-NiCr and WC-Cr3C2-Ni thermally sprayed coatings under tensile bending stress
    Mayrhofer, Erwin
    Janka, Leo
    Mayr, Wolfgang Peter
    Norpoth, Jonas
    Ripoll, Mane Rodriguez
    Groeschl, Martin
    SURFACE & COATINGS TECHNOLOGY, 2015, 281 : 169 - 175
  • [50] Thermal stability of nanostructured Cr3C2-NiCr coatings
    He, JH
    Ice, M
    Schoenung, JM
    Shin, DH
    Lavernia, EJ
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2001, 10 (02) : 293 - 300