Effect of annealing on mechanical properties of silicon carbide sintered with aluminum nitride and scandium oxide

被引:0
|
作者
Shin-Il Ko
Sang-Jin Lee
Myong-Hoon Roh
Wonjoong Kim
Young-Wook Kim
机构
[1] Mokpo National University,Department of Advanced Materials Science and Engineering
[2] The University of Seoul,Department of Materials Science and Engineering
来源
关键词
ceramics; silicon carbide; microstructure; toughness; strength;
D O I
暂无
中图分类号
学科分类号
摘要
Beta-SiC powder samples containing 1 wt.% α-SiC as a seed and 10 vol.% AlN-Sc2O3 as a sintering additive were hot-pressed at 1900 °C for 1 h and subsequently annealed at 2000 °C for 1 h, 3 h and 6 h. When the annealing time was increased, the microstructure changed from equiaxed to elongated grains, which resulted in a self-reinforced microstructure consisting of elongated grains (hexagonal platelet grains in 3-dimensions). The development of a self-reinforced microstructure resulted in significant improvement in toughness. However, the improved toughness was offset by a reduction in strength. The typical fracture toughness and strength of the ceramics annealed for 6 h were 7.3 MPa·m1/2 and ∼500 MPa, respectively.
引用
收藏
页码:149 / 153
页数:4
相关论文
共 50 条
  • [31] Effect of initial α-phase content on microstructure and mechanical properties of sintered silicon carbide
    Kim, YW
    Mitomo, M
    Emoto, H
    Lee, JG
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1998, 81 (12) : 3136 - 3140
  • [32] The effect of oxide, carbide, nitride and boride additives on properties of pressureless sintered SiC: A review
    Khodaei, Mandi
    Yaghobizadeh, Omid
    Alhosseini, S. Hojat Naghavi
    Esmaeeli, Sadeq
    Mousavi, Seyyed Rasool
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (07) : 2215 - 2231
  • [33] Microstructure and mechanical properties of microwave sintered silicon nitride
    Valecillos, MC
    Hirota, M
    Brito, ME
    Hirao, K
    Toriyama, M
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1998, 106 (12) : 1162 - 1166
  • [34] Mechanical and tribological properties of carbon nitride, silicon carbide and silicon nitride coatings
    Leiste, H
    Stüber, M
    Ulrich, S
    Holleck, H
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2000, 31 (08) : 743 - 746
  • [35] Fabrication and mechanical properties of silicon carbide–silicon nitride nanocomposites
    Young–Wook Kim
    M. Mitomo
    Journal of Materials Science, 2000, 35 : 5885 - 5890
  • [36] Control of microstructure and mechanical properties of sintered aluminum nitride through addition of aluminum nitride whiskers
    Kondo, Naoki
    Shimamura, Akihiro
    Hotta, Mikinori
    Shimizu, Hiroki
    Ujihara, Toru
    Ohnishi, Yoshihiro
    JOURNAL OF ASIAN CERAMIC SOCIETIES, 2021, 9 (03): : 1248 - 1254
  • [37] Mechanical properties of carbon, silicon carbide, and boron nitride nanotubes: effect of ionization
    Petrushenko, Igor K.
    Petrushenko, Konstantin B.
    MONATSHEFTE FUR CHEMIE, 2015, 146 (10): : 1603 - 1608
  • [38] Mechanical properties of carbon, silicon carbide, and boron nitride nanotubes: effect of ionization
    Igor K. Petrushenko
    Konstantin B. Petrushenko
    Monatshefte für Chemie - Chemical Monthly, 2015, 146 : 1603 - 1608
  • [39] Heat-resistant silicon carbide with aluminum nitride and erbium oxide
    Kim, YW
    Mitomo, M
    Nishimura, T
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (09) : 2060 - 2064