The nature of stresses in hot-filament chemical vapour deposited diamond thin films on WC substrates

被引:0
|
作者
S CHATTERJEE
A. G EDWARDS
C. S FEIGERLE
机构
[1] Department of Industrial Engineering,Department of Chemistry
[2] The University of Tennessee,undefined
来源
关键词
Carbide; Tungsten; Compressive Stress; Surface Treatment; Tungsten Carbide;
D O I
暂无
中图分类号
学科分类号
摘要
The nature of film stresses in hot-filament chemical vapour deposited (HFCVD) diamond thin films on tungsten carbide substrates, is reported. Commercial WC substrates were subjected to various surface treatments. Subsequently, they were coated with a diamond film and examined for stresses using X-ray diffraction. All but one of the stress measurements indicated various levels of compressive stresses in the film and at the film–substrate interface. These stresses are compared with those obtained by other researchers. Intrinsic film stresses were also computed for diamond films and found to be tensile. WC drills, of 0.125 in. diameter, were also diamond coated and the stress levels measured along drill flanks and flutes. Significant variations were found in these stresses, and the results were analysed from a film–substrate adhesion perspective.
引用
收藏
页码:3355 / 3360
页数:5
相关论文
共 50 条
  • [21] Microwave and hot filament chemical vapour deposition of diamond multilayers on Si and WC-Co substrates
    Kadlecikova, M.
    Vojs, M.
    Breza, J.
    Vesely, M.
    Frgala, Z.
    Michalka, M.
    Matejkova, J.
    Vojackova, A.
    Danis, T.
    Marton, M.
    MICROELECTRONICS JOURNAL, 2007, 38 (01) : 20 - 23
  • [22] Growth and characterization of multilayer hot-filament chemical vapor deposition diamond coatings on WC-Co substrates
    Vieira, Jose
    Contin, Andre
    Fraga, Mariana Amorim
    Corat, Evaldo Jose
    Airoldi, Vladimir Trava
    SURFACE INNOVATIONS, 2019, 7 (01) : 4 - 11
  • [23] Diamond growth on hot-filament chemically vapour-deposited diamond for surface conductive device applications
    Williams, OA
    Jackman, RB
    DIAMOND AND RELATED MATERIALS, 2004, 13 (01) : 166 - 169
  • [24] PLASMA-ETCHED POLYCRYSTALLINE HOT-FILAMENT CHEMICAL-VAPOR-DEPOSITED DIAMOND THIN-FILMS AND THEIR ELECTRICAL CHARACTERISTICS
    LIAW, BY
    STACY, T
    ZHAO, G
    CHARLSON, EJ
    CHARLSON, EM
    MEESE, JM
    PRELAS, MA
    APPLIED PHYSICS LETTERS, 1994, 65 (22) : 2827 - 2829
  • [25] Simultaneous growth of diamond and nanostructured graphite thin films by hot-filament chemical vapor deposition
    Ali, M.
    Urgen, M.
    SOLID STATE SCIENCES, 2012, 14 (01) : 150 - 154
  • [26] Diamond growth with CF4 addition in hot-filament chemical vapour deposition
    Corat, EJ
    TravaAiroldi, VJ
    Leite, NF
    Nono, MCA
    Baranauskas, V
    JOURNAL OF MATERIALS SCIENCE, 1997, 32 (04) : 941 - 947
  • [27] Diamond/WC bilayer formation mechanism by hot-filament CVD
    Neto, M. A.
    Silva, E. L.
    Fernandes, A. J. S.
    Oliveira, F. J.
    Silva, R. F.
    SURFACE & COATINGS TECHNOLOGY, 2012, 206 (13): : 3055 - 3063
  • [28] Analysis and modeling of residual stress in diamond thin film deposited by the hot-filament chemical vapor deposition process
    Seung I. Cha
    Soon H. Hong
    Journal of Materials Research, 2001, 16 : 1953 - 1959
  • [29] Analysis and modeling of residual stress in diamond thin film deposited by the hot-filament chemical vapor deposition process
    Cha, SI
    Hong, SH
    JOURNAL OF MATERIALS RESEARCH, 2001, 16 (07) : 1953 - 1959
  • [30] Structure and properties of polycrystalline diamond thin films grown by hot-filament chemical vapor deposition system
    Pandey, PT
    Vankar, VD
    Gupta, S
    Pradhan, A
    PROCEEDINGS OF THE ELEVENTH INTERNATIONAL WORKSHOP ON THE PHYSICS OF SEMICONDUCTOR DEVICES, VOL 1 & 2, 2002, 4746 : 1170 - 1173