Effect of Strontium and Phosphorus on Eutectic Al-Si Nucleation and Formation of β-Al5FeSi in Hypoeutectic Al-Si Foundry Alloys

被引:0
|
作者
Y.H. Cho
H.-C. Lee
K.H. Oh
A.K. Dahle
机构
[1] Seoul National University,Department of Materials Science and Engineering
[2] The University of Queensland,Division of Materials Engineering
关键词
Eutectic Silicon; Unmodified Alloy; Aluminum Phosphide; Eutectic Nucleation;
D O I
暂无
中图分类号
学科分类号
摘要
The present investigation was carried out on hypoeutectic Al-Si alloys containing two levels of Fe, 0.5 and 1.1 wt pct, and Sr in the range of 30 to 500 ppm. The addition of Sr in excess of 100 ppm significantly reduced the number of eutectic grains and also resulted in the formation of polygonal-shaped Al2Si2Sr intermetallics. Transmission electron microscopy studies revealed that the Al2Si2Sr phase surrounded the P-rich particles. This may suggest that the otherwise potent nuclei for the Al-Si eutectic, aluminum phosphide (AlP), become poisoned or deactivated by the formation of the Al2Si2Sr phase around the particles. At the high-Fe level (1.1 wt pct Fe), pre-eutectic formation of β-Al5FeSi platelets further reduced the number of eutectic Al-Si nucleation events. It is proposed that both eutectic silicon and β-Al5FeSi are preferentially nucleated on AlP particles. Nucleation of eutectic silicon, therefore, becomes more difficult when it is preceded by the formation of Al2Si2Sr or β-Al5FeSi, because fewer nuclei are available to nucleate silicon. Addition of up to 60 ppm P to the alloys increased the formation temperature of the β-Al5FeSi platelets but did not significantly alter the size, whereas the addition of Sr decreased the β-Al5FeSi nucleation temperature by reducing the potency of the AlP particles.
引用
收藏
页码:2435 / 2448
页数:13
相关论文
共 50 条
  • [41] Nucleation and Growth of Eutectic Si in Al-Si Alloys with Na Addition
    J. H. Li
    J. Barrirero
    M. Engstler
    H. Aboulfadl
    F. Mücklich
    P. Schumacher
    Metallurgical and Materials Transactions A, 2015, 46 : 1300 - 1311
  • [42] EFFECT OF STRONTIUM ON VISCOSITY AND LIQUID STRUCTURE OF Al-Si EUTECTIC ALLOYS
    Shankar, Sumanth
    Prakash, Srirangam V. S.
    Malik, Minhajuddin
    Jeyakumar, Manickaraj
    Walker, Michael J.
    Hamed, Mohamed
    SHAPE CASTING: 3RD INTERNATIONAL SYMPOSIUM 2009, 2009, : 173 - +
  • [43] Determination of eutectic growth mode in hypoeutectic Al-Si foundry alloys by EBSP investigations in SEM
    Dahle, AK
    Hjelen, J
    Arnberg, L
    ELECTRON MICROSCOPY 1998, VOL 2: MATERIALS SCIENCE 1, 1998, : 135 - 136
  • [44] Nucleation and Growth of Eutectic Si in Al-Si Alloys with Na Addition
    Li, J. H.
    Barrirero, J.
    Engstler, M.
    Aboulfadl, H.
    Muecklich, F.
    Schumacher, P.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (03): : 1300 - 1311
  • [45] THE EFFECT OF ROTATION ON THE EUTECTIC PHASE IN HYPOEUTECTIC AL-SI ALLOY
    BASAK, PS
    RAY, BC
    CHAKRABARTY, I
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1991, 10 (06) : 313 - 315
  • [46] Fatigue of eutectic Al-Si alloys
    Ecole Nationale Superieure des Mines, Saint-Etienne, France
    Materials Science Forum, 1996, 217-222 (pt 3): : 1343 - 1348
  • [47] Modification of hypoeutectic Al-Si alloys with scandium
    Prukkanon, Wattanachai
    Srisukhumbowornchai, Nakorn
    Limmaneevichitr, Chaowalit
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 477 (1-2) : 454 - 460
  • [48] Aluminium phosphide as a eutectic grain nucleus in hypoeutectic Al-Si alloys
    Nogita, K
    McDonald, SD
    Tsujimoto, K
    Yasuda, K
    Dahle, AK
    JOURNAL OF ELECTRON MICROSCOPY, 2004, 53 (04): : 361 - 369
  • [49] Fatigue of eutectic Al-Si alloys
    MadelaineDupuich, O
    Stolarz, J
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 1343 - 1348
  • [50] HARDNESS OF AL-SI EUTECTIC ALLOYS
    VNUK, F
    SAHOO, M
    VANDEMERWE, R
    SMITH, RW
    JOURNAL OF MATERIALS SCIENCE, 1979, 14 (04) : 975 - 982