Titanium-based films deposited using a Nd:YAG pulsed laser

被引:0
|
作者
B. Major
R. Ebner
P. Zieba
W. Wolczynski
机构
[1] Institute of Metallurgy and Materials Science,
[2] Polish Academy of Sciences,undefined
[3] Reymonta Street 25,undefined
[4] 30-059 Cracow,undefined
[5] Poland (Fax: +48-12/637-2192,undefined
[6] E-mail: nmmajor@al.imim-pan.krakow.pl),undefined
[7] Montanuniversität Leoben,undefined
[8] Franz-Josef-Strasse 18,undefined
[9] 8700 Leoben,undefined
[10] Austria (Fax: +43-3842/402-737,undefined
[11] E-mail: ebner-r@unileoben.ac.at),undefined
来源
Applied Physics A | 1999年 / 69卷
关键词
PACS: 68.55.a.Jk; Nq,81.15;
D O I
暂无
中图分类号
学科分类号
摘要
Complex examinations were performed of the structure of films of metallic titanium, titanium nitride and titanium oxide deposited by means of PLD with a Nd:YAG laser. The influence of the deposition parameters on the film morphology was examined. The films revealed a nano-structure of good quality. A new tetragonal Ti(N) phase was revealed in the deposition of metallic titanium in a reactive chamber with an argon atmosphere. The TiN phase was formed during deposition of titanium nitride, independently of the nitrogen flow in the chamber. The transition of oxides from Ti2O via TiO to TiO2 was observed with an increasing flow of oxygen in the chamber for deposition of titanium oxide. TEM examinations of the microstructure in cross-sections of the film revealed a micro- columnar structure. All the examined films were characterised by a strong axial crystallographic preferred orientation on the basis of the measured pole figures. The <001> axial texture was identified within the deposited metallic titanium for the Ti(N) tetragonal phase as well as for the TiO oxide, while the <111> texture was observed in the case of TiN nitride. Measurements of the residual stresses of the first order in the TiN phase, by using the X-ray sin2ψ method, showed stress levels of -5000 to -7000 MPa. The residual stresses measured in the substrate of ferritic steel were about -150 MPa.
引用
收藏
页码:S921 / S923
相关论文
共 50 条
  • [41] Comparison of surface films formed on titanium by pulsed Nd:YAG laser irradiation at different powers and wavelengths in nitrogen atmosphere
    Ohtsu, Naofumi
    Kodama, Kenji
    Kitagawa, Kuniyuki
    Wagatsuma, Kazuaki
    APPLIED SURFACE SCIENCE, 2010, 256 (14) : 4522 - 4526
  • [42] MAGNETISM AND STRUCTURE OF YBACUO SUPERCONDUCTING FILMS DEPOSITED IN UNUSUAL GEOMETRIES USING ND-YAG LASER
    KOGA, T
    MOON, BM
    ZAKHARCHENKO, I
    RAO, KV
    MEDELIUS, H
    IEEE TRANSACTIONS ON MAGNETICS, 1993, 29 (06) : 3601 - 3603
  • [43] DEPOSITION OF TITANIUM-BASED FILMS BY LASER-ASSISTED THERMAL CVD OF TITANIUM TETRACHLORIDE
    ALEXANDRESCU, R
    CIREASA, R
    DRAGNEA, B
    MORJAN, I
    VOICU, I
    ANDREI, A
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C3): : 265 - 272
  • [44] UV laser micromachining of piezoelectric ceramic using a pulsed Nd:YAG laser
    Zeng, DW
    Li, K
    Yung, KC
    Chan, HLW
    Choy, CL
    Xie, CS
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2004, 78 (03): : 415 - 421
  • [45] Pulsed Nd:YAG laser depositions of ITO and DLC films for OLED applications
    Yong, T. K.
    Yap, S. S.
    Safran, Gyorgy
    Tou, T. Y.
    APPLIED SURFACE SCIENCE, 2007, 253 (11) : 4955 - 4959
  • [46] UV laser micromachining of piezoelectric ceramic using a pulsed Nd:YAG laser
    D.W. Zeng
    K. Li
    K.C. Yung
    H.L.W. Chan
    C.L. Choy
    C.S. Xie
    Applied Physics A, 2004, 78 : 415 - 421
  • [47] Nd:YAG pulsed laser welding of dissimilar metals of titanium alloy to stainless steel
    Y. Zhang
    D. Q. Sun
    X. Y. Gu
    H. M. Li
    The International Journal of Advanced Manufacturing Technology, 2018, 94 : 1073 - 1085
  • [48] Polarity of homoepitaxial ZnO films grown by Nd:YAG pulsed laser deposition
    Masuda, Tatsuya
    Sato, Toshihiro
    Lippmaa, Mikk
    Dazai, Takuro
    Sekine, Norihiko
    Hosako, Iwao
    Koinuma, Hideomi
    Takahashi, Ryota
    JOURNAL OF APPLIED PHYSICS, 2024, 136 (09)
  • [49] Chromium carbide thin films synthesized by pulsed Nd:YAG laser deposition
    Suda, Y
    Kawasaki, H
    Terajima, R
    Emura, M
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1999, 38 (6A): : 3619 - 3621
  • [50] Characterization of crystalline TiC films grown by pulsed Nd:YAG laser deposition
    Suda, Yoshiaki
    Kawasaki, Hiroharu
    Cho, Choong-Rae
    Grishin, Alex
    Rao, K.V.
    Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 2000, 39 (7 B): : 4575 - 4576