Determination of Interfacial Fracture Toughness of Thermal Spray Coatings by Indentation

被引:0
|
作者
Yasuhiro Yamazaki
Masayuki Arai
Yukio Miyashita
Hiroyuki Waki
Masato Suzuki
机构
[1] Niigata Institute of Technology,Mechanical and Control Engineering
[2] Tokyo University of Science,Mechanical Engineering
[3] Nagaoka University of Technology,Mechanical Engineering
[4] Iwate University,Mechanical Engineering
[5] The National Institute of Advanced Industrial Science and Technology,undefined
来源
关键词
indentation test; interfacial fracture toughness; thermal spray coatings; test standardization;
D O I
暂无
中图分类号
学科分类号
摘要
Adhesion is an important and basic property for thermal spray coatings. The standard tensile test method “ISO 14916” is usually used to evaluate the adhesive strength of coatings. On the other hand, the indentation test method has some advantages to evaluate the interfacial fracture toughness as the adhesive strength, arising from the following reasons: the test procedure and the specimen preparation are easy in comparison with the typical testing method. Collaborative research has been conducted by “Committee on Standard Development” in the Japan Thermal Spray Society to establish a standard test method for evaluating interfacial fracture toughness of thermal spray coatings using a conventional Vickers indenter. This article reports the differences among collaborators in round-robin tests performed in this committee and discusses the validity of the test method and test conditions with respect to the test results and finite element analyses. Comparison among collaborators reveals that interfacial fracture toughness can be obtained with a small scattering from the indentation test under constraints found on the basis of the results.
引用
收藏
页码:1358 / 1365
页数:7
相关论文
共 50 条
  • [21] Indentation of Metallic and Cermet Thermal Spray Coatings
    Choi, W. B.
    Prchlik, L.
    Sampath, S.
    Gouldstone, A.
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2009, 18 (01) : 58 - 64
  • [22] Indentation of Metallic and Cermet Thermal Spray Coatings
    W.B. Choi
    L. Prchlik
    S. Sampath
    A. Gouldstone
    Journal of Thermal Spray Technology, 2009, 18 : 58 - 64
  • [23] Role of impact on determination of interfacial toughness measurement by indentation for thermal barrier coating systems
    Ekici, B
    SURFACE ENGINEERING, 2005, 21 (5-6) : 456 - 462
  • [24] Application of the interfacial indentation test for adhesion toughness determination
    Chicot, D
    Araujo, P
    Horny, N
    Tricoteaux, A
    Lesage, J
    SURFACE & COATINGS TECHNOLOGY, 2005, 200 (1-4): : 174 - 177
  • [25] Indentation characterization of fracture toughness and interfacial strength of PECVD nitrides after rapid thermal annealing
    Yan, H-Y
    Ou, K-S
    Chen, K-S
    MICROELECTROMECHANICAL SYSTEMS - MATERIALS AND DEVICES, 2008, 1052 : 59 - 64
  • [26] Interfacial fracture toughness for film on substrate determined by indentation method
    Lee, Soohyun
    Kim, Jinkwang
    Kim, Sunam
    Cho, Sangbong
    Yun, Jondo
    Mechanical Behavior of Materials X, Pts 1and 2, 2007, 345-346 : 801 - 804
  • [27] Interface fracture toughness and fracture mechanisms of thermal barrier coatings investigated by indentation test and acoustic emission technique
    韩纪层
    郭平
    罗建霞
    张志超
    李强
    China Welding, 2016, 25 (03) : 63 - 70
  • [28] Indentation fracture and toughness assessment for thin optical coatings on glass
    Chen, J.
    Bull, S. J.
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2007, 40 (18) : 5401 - 5417
  • [29] Indentation tests to determine the fracture toughness of nickel phosphorus coatings
    Roman, A
    Chicot, D
    Lesage, J
    SURFACE & COATINGS TECHNOLOGY, 2002, 155 (2-3): : 161 - 168
  • [30] Influence of Fracture Toughness and Microhardness on the Erosive Wear of Cermet Coatings Deposited by Thermal Spray
    Miguel Reyes Mojena
    Mario Sánchez Orozco
    Hipólito Carvajal Fals
    Valtair Antonio Ferraresi
    Carlos Roberto Camello Lima
    Metallurgical and Materials Transactions A, 2017, 48 : 2511 - 2518