Photocatalytic degradation of Novacron blue and Novacron yellow textile dyes by the TiO2/palygorskite nanocomposite

被引:0
|
作者
Mikaely Lizandra Moreira de Assis
Elmar Damasceno Junior
Janiele Mayara Ferreira de Almeida
Isabel do Nascimento Silva
Rodrigo Victor Barbosa
Lamara Maciel dos Santos
Elizete Faustino Dias
Nedja Suely Fernandes
Carlos Alberto Martinez-Huitle
机构
[1] Campus Universitário Lagoa Nova,Universidade Federal do Rio Grande do Norte, Instituto de Química, Laboratório de Química Analítica e Meio Ambiente—LAQUAM
[2] Campus Universitário Lagoa Nova,Universidade Federal do Rio Grande do Norte, Instituto de Química, Laboratório de Eletroquímica Ambiental e Aplicada—LEAA
关键词
Textile dyes; Novacron blue; Novacron yellow; Photocatalysis; Titanium dioxide; Palygorskite;
D O I
暂无
中图分类号
学科分类号
摘要
The photocatalytic discoloration of industrial dyes, Novacron blue (NB) and Novacron yellow (NY), was investigated using composites based on TiO2 and natural palygorskite (Pal-Ti10 and Pal-Ti30). The method consisted of synthesizing the composites starting from a physical mixture of TiO2 and natural palygorskite in the presence of alcohol, for impregnation through calcination under conditions of temperature equal to 450 °C and atmospheric air. The characterization techniques used in this work were FTIR, XRD, XRF, SEM, particle size analysis and zeta potential. The photocatalysis for the NB dye was investigated through the application of a factorial 24 experimental design, aiming at the best experimental conditions and finally applying them in another NY industrial dye. The investigated concentrations of NB were 10 ppm and 30 ppm, the composites were synthesized using 10 and 30% (p/p) of titanium dioxide in palygorskite, the two pH values were 2.0 and 6.0 and the light intensities 9 and 18 W were used. Tests performed at pH 2.0, Pal-Ti30 composite, power 18 W and 10 ppm of dye showed 100% color removal of both dyes in 90 min. The bleaching process followed the pseudo-first order kinetic model, and the apparent constants (Kapp) were 0.0216 min−1 and 0.0193 min−1 for NB and NY dyes, respectively. The results of total organic carbon (TOC) showed mineralization of 61.70% and 58.06% for NB and NY, respectively, in 90 min of treatment, and the by-products were detected by GC-MS.
引用
收藏
页码:64440 / 64460
页数:20
相关论文
共 50 条
  • [31] Ultrasmall Plasmonic Nanoparticles Decorated Hierarchical Mesoporous TiO2 as an Efficient Photocatalyst for Photocatalytic Degradation of Textile Dyes
    Vandarkuzhali, S. Anbu Anjugam
    Pugazhenthiran, N.
    Mangalaraja, R. V.
    Sathishkumar, P.
    Viswanathan, B.
    Anandan, S.
    ACS OMEGA, 2018, 3 (08): : 9834 - 9845
  • [32] Superior photocatalytic degradation of azo dyes in aqueous solutions using TiO2/SrTiO3 nanocomposite
    Karimi L.
    Zohoori S.
    Journal of Nanostructure in Chemistry, 2013, 3 (1)
  • [33] Photocatalytic Degradation of Dyes in Water Using TiO2/Hydroxyapatite Composites
    Huan-re Han
    Xin Qian
    Ye Yuan
    Mi Zhou
    Yu-long Chen
    Water, Air, & Soil Pollution, 2016, 227
  • [34] Solar photocatalytic degradation of eight commercial dyes in TiO2 suspension
    Wang, YZ
    WATER RESEARCH, 2000, 34 (03) : 990 - 994
  • [35] Parameters affecting the photocatalytic degradation of dyes using TiO2: a review
    Reza K.M.
    Kurny A.
    Gulshan F.
    Applied Water Science, 2017, 7 (4) : 1569 - 1578
  • [36] Rules of photocatalytic oxidation degradation of dyes in TiO2/UV system
    Xiao, Jun-Xia
    Wei, Chao-Hai
    Hu, Ji-Jie
    Ren, Yuan
    Wu, Chao-Fei
    Huanan Ligong Daxue Xuebao/Journal of South China University of Technology (Natural Science), 2008, 36 (03): : 77 - 82
  • [37] Photocatalytic Degradation of Dyes in Water Using TiO2/Hydroxyapatite Composites
    Han, Huan-re
    Qian, Xin
    Yuan, Ye
    Zhou, Mi
    Chen, Yu-long
    WATER AIR AND SOIL POLLUTION, 2016, 227 (12):
  • [38] Photocatalytic degradation of Azure and Sudan dyes using nano TiO2
    Aarthi, T.
    Narahari, Prashanthi
    Madras, Giridhar
    JOURNAL OF HAZARDOUS MATERIALS, 2007, 149 (03) : 725 - 734
  • [39] Adsorption of organic dyes on TiO2 and its effect on photocatalytic degradation
    Yi, Xiao-Yun
    Li, Xin-Jun
    Gu, Guo-Bang
    Shi, Lin
    Huanan Ligong Daxue Xuebao/Journal of South China University of Technology (Natural Science), 2002, 30 (09):
  • [40] Fabrication and photocatalytic performance of electrospun PVA/silk/TiO2 nanocomposite textile
    Wu, Ming-Chung
    Chan, Shun-Hsiang
    Lin, Ting-Han
    FUNCTIONAL MATERIALS LETTERS, 2015, 8 (03)