Wetting and reaction of Sn-2.8Ag-0.5Cu-1.0Bi solder with Cu and Ni substrates

被引:0
|
作者
M. J. Rizvi
Y. C. Chan
C. Bailey
H. Lu
M. N. Islam
B. Y. Wu
机构
[1] City University of Hong Kong,Department of Electronic Engineering
[2] University of Greenwich,School of Computing and Mathematical Sciences
来源
关键词
Wettability; Sn-2.8Ag-0.5Cu-1.0Bi; wetting force; contact angle; flux; surface tension; finite element modeling; intermetallic compounds;
D O I
暂无
中图分类号
学科分类号
摘要
The wettability of newly developed Sn-2.8Ag-0.5Cu-1.0Bi lead-free solder on Cu and Ni substrates was assessed through the wetting balance tests. The wettability assessment parameters such as contact angle (ϑc) and maximum wetting force (Fw) were documented for three solder bath temperatures with three commercial fluxes, namely, no-clean (NC), nonactivated (R), and water-soluble organic acid flux (WS). It was found that the lead-free Sn-2.8Ag-0.5Cu-1.0Bi solder exhibited less wetting force, i.e., poorer wettability, than the conventional Sn-37Pb solder for all flux types and solder bath temperatures. The wettability of Sn-2.8Ag-0.5Cu-1.0Bi lead-free solder on Cu substrate was much higher than that on Ni substrate. Nonwetting for Sn-2.8Ag-0.5Cu-1.0Bi and Sn-Pb solders on Ni substrate occurred when R-type flux was used. A model was built and simulations were performed for the wetting balance test. The simulation results were found very close to the experimental results. It was also observed that larger values of immersion depth resulted in a decrease of the wetting force and corresponding meniscus height, whereas the increase in substrate perimeter enhanced the wettability. The wetting reactions between the solder and Cu/Ni substrates were also investigated, and it was found that Cu atoms diffused into the solder through the intermetallic compounds (IMCs) much faster than did the Ni atoms. Rapid formation of IMCs inhibited the wettability of Sn-2.8Ag-0.5Cu-1.0Bi solder compared to the Sn-Pb solder.
引用
收藏
页码:1115 / 1122
页数:7
相关论文
共 50 条
  • [31] Precipitation and coarsening of bismuth plates in Sn-Ag-Cu-Bi and Sn-Cu-Ni-Bi solder joints
    Belyakov, S. A.
    Xian, J.
    Zeng, G.
    Sweatman, K.
    Nishimura, T.
    Akaiwa, T.
    Gourlay, C. M.
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2019, 30 (01) : 378 - 390
  • [32] Refinement of the β-Sn Grains in Ni-Doped Sn-3.0Ag-0.5Cu Solder Joints with Cu-Based and Ni-Based Substrates
    Chou, Tzu-Ting
    Chen, Wei-Yu
    Fleshman, Collin Jordon
    Duh, Jenq-Gong
    JOURNAL OF ELECTRONIC MATERIALS, 2018, 47 (05) : 2911 - 2919
  • [33] Refinement of the β-Sn Grains in Ni-Doped Sn-3.0Ag-0.5Cu Solder Joints with Cu-Based and Ni-Based Substrates
    Tzu-Ting Chou
    Wei-Yu Chen
    Collin Jordon Fleshman
    Jenq-Gong Duh
    Journal of Electronic Materials, 2018, 47 : 2911 - 2919
  • [34] Effect of Yttrium on the Fracture Strength of the Sn-1.0Ag-0.5Cu Solder Joints
    Hyelim Choi
    Wayne D. Kaplan
    Heeman Choe
    Journal of Electronic Materials, 2016, 45 : 3259 - 3262
  • [35] Modification of Sn–1.0Ag–0.5Cu solder using nickel and boron
    Jun-Feng Qu
    Jun Xu
    Qiang Hu
    Fu-Wen Zhang
    Shao-Ming Zhang
    Rare Metals, 2015, 34 : 783 - 788
  • [36] Effect of Yttrium on the Fracture Strength of the Sn-1.0Ag-0.5Cu Solder Joints
    Choi, Hyelim
    Kaplan, Wayne D.
    Choe, Heeman
    JOURNAL OF ELECTRONIC MATERIALS, 2016, 45 (07) : 3259 - 3262
  • [37] Modification of Sn–1.0Ag–0.5Cu solder using nickel and boron
    Jun-Feng Qu
    Jun Xu
    Qiang Hu
    Fu-Wen Zhang
    Shao-Ming Zhang
    RareMetals, 2015, 34 (11) : 783 - 788
  • [38] Effects of In addition on the properties of Sn-4Ag-0.5Cu-3Bi-0.05Ni solder
    Gao, Caihong
    Qiao, Yuanyuan
    Zhao, Ning
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2024, 35 (19)
  • [39] Investigation of Wetting Behavior of Sn-3Ag-0.5Cu Solder Paste to BGA Solder Ball
    Yahya, Maryam Husna
    Nakamura, Keisuke
    Shohji, Ikuo
    Housen, Toshihiro
    Yamamoto, Yumi
    Kaga, Yoshio
    2012 35TH IEEE/CPMT INTERNATIONAL ELECTRONICS MANUFACTURING TECHNOLOGY SYMPOSIUM (IEMT), 2012,
  • [40] Interfacial reaction of Sn-Ag-Cu-Ni solder/Cu joints by laser process
    Nishikawa, Hiroshi
    Matsunobu, Ryo
    2018 7TH ELECTRONIC SYSTEM-INTEGRATION TECHNOLOGY CONFERENCE (ESTC), 2018,