Surface Selective Oxide Reduction During the Intercritical Annealing of Medium Mn Steel

被引:0
|
作者
Kyoung Rae Jo
Lawrence Cho
Jong Han Oh
Myoung Soo Kim
Ki Cheol Kang
Bruno C. De Cooman
机构
[1] Pohang University of Science and Technology (POSTECH),Materials Design Laboratory, Graduate Institute of Ferrous Technology (GIFT)
[2] POSCO,Technical Research Laboratories
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Third generation advanced high-strength steels achieve an excellent strength–ductility balance using a cost-effective alloy composition. During the continuous annealing of medium Mn steel, the formation of an external selective oxide layer of MnO has a negative impact on the coating quality after galvanizing. A procedure to reduce the selective oxide was therefore developed. It involves annealing in the temperature range of 1073 K to 1323 K (800 °C to 1050 °C) in a HNx gas atmosphere. Annealing at higher temperatures and the use of larger H2 volume fractions are shown to make the gas atmosphere reducing with respect to MnO. The reduction of the surface MnO layer was observed by SEM, GDOES, and cross-sectional TEM analysis.
引用
收藏
页码:3635 / 3641
页数:6
相关论文
共 50 条
  • [31] Modelling and experimental validation of austenite growth from As-quenched martensite during intercritical annealing of a medium-Mn steel
    Lin, Guanqiang
    Lan, Huifang
    Du, Linxiu
    JOURNAL OF MATERIALS SCIENCE, 2021, 56 (34) : 19165 - 19179
  • [32] Modelling and experimental validation of austenite growth from As-quenched martensite during intercritical annealing of a medium-Mn steel
    Guanqiang Lin
    Huifang Lan
    Linxiu Du
    Journal of Materials Science, 2021, 56 : 19165 - 19179
  • [33] Investigation on the Microstructural Evolution in a Medium-Mn steel (X10Mn5) after Intercritical Annealing
    Steineder, K.
    Schneider, R.
    Krizan, D.
    Beal, C.
    Sommitsch, C.
    HTM-JOURNAL OF HEAT TREATMENT AND MATERIALS, 2015, 70 (01): : 19 - 25
  • [34] FORMATION OF MEDIUM CARBON TRIP STEEL MICROSTRUCTURE DURING ANNEALING IN THE INTERCRITICAL TEMPERATURE RANGE
    Kokosza, A.
    Pacyna, J.
    ARCHIVES OF METALLURGY AND MATERIALS, 2014, 59 (03) : 1017 - 1022
  • [35] Stabilizing austenite via intercritical Mn partitioning in a medium Mn steel
    Hu, Baojia
    Zheng, Qinyuan
    Lu, Yi
    Jia, Chunni
    Liang, Tian
    Zheng, Chengwu
    Li, Dianzhong
    SCRIPTA MATERIALIA, 2023, 225
  • [36] Mn Diffusion at Early Stage of Intercritical Annealing of 5Mn Steel
    Xi-nan LUO
    Xiao-yan ZHONG
    Hai-wen LUO
    Hui-hua ZHOU
    Cun-yu WANG
    Jie SHI
    Journal of Iron and Steel Research(International), 2015, 22 (11) : 1015 - 1019
  • [37] Impact of intercritical annealing temperature and strain state on mechanical stability of retained austenite in medium Mn steel
    Yang, Yong-Gang
    Mi, Zhen-Li
    Xu, Mei
    Xiu, Qi
    Li, Jun
    Jiang, Hai-Tao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 725 : 389 - 397
  • [38] Influence of intercritical annealing to obtain austenite in 3rd generation AHSS medium Mn steel
    Solana-Reyes, Y.
    Bocanegra-Hueramo, A. J.
    Garnica-Gonzalez, P.
    Pacheco-Cedeno, J. S.
    Cruz-Hernandez, J. J.
    MRS ADVANCES, 2024, : 121 - 125
  • [39] Two-Step Intercritical Annealing to Eliminate Luders Band in a Strong and Ductile Medium Mn Steel
    Ma, Jiawei
    Lu, Qi
    Sun, Li
    Shen, Yao
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (10): : 4404 - 4408
  • [40] Mn Diffusion at Early Stage of Intercritical Annealing of 5Mn Steel
    Luo, Xi-nan
    Zhong, Xiao-yan
    Luo, Hai-wen
    Zhou, Hui-hua
    Wang, Cun-yu
    Shi, Jie
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2015, 22 (11) : 1015 - 1019