Hot Corrosion Behavior of Hf-Doped NiAl Coating in the Mixed Salt of Na2SO4 + K2SO4 at 900 °C

被引:0
|
作者
W. L. Zhang
W. Li
L. B. Fu
X. Peng
J. Sun
S. M. Jiang
J. Gong
C. Sun
机构
[1] Chinese Academy of Sciences,Shi
[2] University of Science and Technology of China,Changxu Innovation Center for Advanced Materials, Institute of Metal Research
[3] Qilu University of Technology (Shandong Academy of Sciences),School of Materials Science and Engineering
关键词
Hot corrosion; Hafnium; Oxide scale; Titanium; Sulfide;
D O I
暂无
中图分类号
学科分类号
摘要
The hot corrosion behavior of the NiAl coating and the 5Hf-NiAl coating induced by mixed salt at 900 °C was investigated. Comparing with the NiAl coating, the 5Hf-NiAl coating exhibited superior hot corrosion resistance because the addition of Hf promoted the formation of protective oxide scale and reduced the growth rate of oxide scale. Therefore, internal sulfides were not present in the 5Hf-NiAl coating after hot corrosion for 140 h. Cr exhibited different distribution in the two coatings since the addition of Hf changed the hot corrosion process of the coating. Hf and Ti in the 5Hf-NiAl coating trapped and captured sulfur, preventing the penetration of sulfur into the coating. The hot corrosion mechanism of the two coating and the effects of Hf on this process were discussed in this work.
引用
收藏
页码:1409 / 1420
页数:11
相关论文
共 50 条
  • [31] A thermodynamic model for high temperature corrosion applications: The (Na2SO4 + K2SO4 + ZnSO4 + PbSO4) system
    Jin, Liling
    Lindberg, Daniel
    Tsuchiyama, Yoshihiko
    Robelin, Christian
    CHEMICAL ENGINEERING SCIENCE, 2022, 260
  • [32] Study on electrochemical performance of activated carbon in aqueous Li2SO4, Na2SO4 and K2SO4 electrolytes
    Qu, Q. T.
    Wang, B.
    Yang, L. C.
    Shi, Y.
    Tian, S.
    Wu, Y. P.
    ELECTROCHEMISTRY COMMUNICATIONS, 2008, 10 (10) : 1652 - 1655
  • [33] A method for investigation of hot corrosion by gaseous Na2SO4
    Knutsson, Pavleta
    Lai, Haiping
    Stiller, Krystyna
    CORROSION SCIENCE, 2013, 73 : 230 - 236
  • [34] VISCOSITY CALCULATIONS FOR K2SO4 AND NA2SO4 SOLUTIONS FROM NUCLEAR MAGNETIC RESONANCE DATA
    GRITSUS, BV
    KUSHCHEN.VV
    MISHCHEN.KP
    ZHURNAL PRIKLADNOI KHIMII, 1970, 43 (12) : 2741 - &
  • [35] Solubility of salicylic acid in water plus salt (NaCl, KCl, NaBr, Na2SO4 and K2SO4) at 293.5-313.3 K
    Pires, Ricardo F.
    Franco, Moilton R., Jr.
    FLUID PHASE EQUILIBRIA, 2012, 330 : 48 - 51
  • [36] Effect of Cold Working on Hot Corrosion Behavior of 9 Cr-1 Mo Ferritic Steel in 75 wt% Na2SO4+25 wt% K2SO4 Molten Salt Environment at 900 A°C
    Shukla, Amarish K.
    Gond, Dinesh
    Puri, D.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (05) : 1049 - 1057
  • [37] Hot corrosion of Ti3SiC2-based ceramic in molten Na2SO4 at 900 °C and 1000 °C
    Liu, GM
    Li, MS
    Zhou, YC
    Zhang, YM
    ACTA METALLURGICA SINICA, 2002, 38 (04) : 417 - 420
  • [38] Corrosion behavior of thermally sprayed WC coating in Na2SO4 aqueous solution
    Takeda, M
    Morihiro, N
    Ebara, R
    Harada, Y
    Wang, RG
    Kido, M
    MATERIALS TRANSACTIONS, 2002, 43 (11) : 2860 - 2865
  • [39] Hot corrosion behavior of AlCuFeCr quasicrystalline coating on titanium alloy with the mixture of NaCl and Na2SO4 deposit
    Wang, Fengfeng
    Zhou, Chungen
    Gong, Shengkai
    Xu, Huibin
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 2313 - +
  • [40] Study on the Solubility of the Aqueous Quaternary System Li2SO4 + Na2SO4 + K2SO4 + H2O at 273.15 K
    Zeng, Ying
    Lin, Xiaofeng
    Yu, Xudong
    JOURNAL OF CHEMICAL AND ENGINEERING DATA, 2012, 57 (12): : 3672 - 3676