Shear and extensional rheometry of PA6 reinforced with polyacrylic nanoparticles

被引:0
|
作者
Estefania Huitrón-Rattinger
Angel Romo-Uribe
机构
[1] Universidad Nacional Autonoma de Mexico,Laboratorio de Nanopolimeros y Coloides, Instituto de Ciencias Fisicas
来源
Polymer Bulletin | 2013年 / 70卷
关键词
PA6; Nanocomposites; Rheology; Extensional viscosity;
D O I
暂无
中图分类号
学科分类号
摘要
Shear and extensional rheometry was carried out on polyamide 6 (PA6) reinforced with crosslinked polyacrylic nanoparticles (PNPs) with mean size of 8 nm. The PNPs were dispersed into a commercial, injection grade, PA6 matrix by melt extrusion, at a concentration of 3 wt%. Thermal analysis showed that the PNPs did not influence the melting and decomposition temperature of the polymer matrix. However, grafting of maleic anhydride to the PNPs (denoted PNP-g-MA) increased the decomposition temperature. On the other hand, X-ray scattering and small-angle light scattering showed that the degree of crystallinity and crystal size were reduced, relative to the neat PA6, i.e., the PNPs disrupted the ordering of the polymer chains. The shear rheological properties showed that the PA6/PNP nanocomposites exhibited a linear viscoelastic behavior. Small-strain oscillatory shear showed that PA6 exhibited a predominantly viscous behavior. However, addition of PNPs induced a predominantly elastic behavior, as measured by the mechanical damping tan δ (=G″/G′), and increased the zero-shear viscosity. The increase in melt elasticity and viscosity was greater for the PA6/PNP-g-MA nanocomposite. Extensional rheometry experiments demonstrated that when PNPs were added to PA6, they induced smaller extensional viscosity, ηext, values in the matrix, at low strain rates. However, at higher strain rates the PNPs induced a strain hardening behavior. Whereas the neat polymer melt rapidly broke under extensional flow, the PA6/PNP nanocomposites first exhibited lower ηext than the neat PA6, and then ηext rapidly increased before breaking, i.e. a strain hardening behavior. The higher melt elasticity of the molten PA6 nanocomposites appears to arise from a jamming effect promoted by the PNPs.
引用
收藏
页码:2547 / 2567
页数:20
相关论文
共 50 条
  • [41] Evaluation of Tribological Properties of Carbon Fiber-Reinforced PA6 Composites
    Li, J.
    Xia, Y. C.
    [J]. POLYMER COMPOSITES, 2010, 31 (03) : 536 - 542
  • [42] Friction welding for the manufacturing of PA6 and ABS structures reinforced with Fe particles
    Kumar, Ranvijay
    Singh, Rupinder
    Ahuja, I. P. S.
    Amendola, Ada
    Penna, Rosa
    [J]. COMPOSITES PART B-ENGINEERING, 2018, 132 : 244 - 257
  • [43] Tribological Investigation of MC PA6 Reinforced by Boron Nitride of Single Layer
    Bingli Pan
    Ning Li
    Guangcheng Chu
    Fengjun Wei
    Jichun Liu
    Junkai Zhang
    Yongzhen Zhang
    [J]. Tribology Letters, 2014, 54 : 161 - 170
  • [44] Fabrication and characterization of three-layer nanofibrous yarn (PA6/PU/PA6)
    Pejman Sohanaki
    Elaheh Ahamadloo
    Ali Akbar Gharehaghaji
    Reza M. A. Malek
    [J]. Polymer Bulletin, 2022, 79 : 7245 - 7264
  • [45] Mechanical strength analysis of almond skin reinforced PA6 metamaterial structures
    Mankotia K.
    Chohan J.S.
    Singh R.
    [J]. Materials Today: Proceedings, 2022, 68 : 1187 - 1192
  • [46] Tribological Investigation of MC PA6 Reinforced by Boron Nitride of Single Layer
    Pan, Bingli
    Li, Ning
    Chu, Guangcheng
    Wei, Fengjun
    Liu, Jichun
    Zhang, Junkai
    Zhang, Yongzhen
    [J]. TRIBOLOGY LETTERS, 2014, 54 (02) : 161 - 170
  • [47] Confined crystallization phenomena in immiscible polymer blends with dispersed micro- and nanometer sized PA6 droplets, part 1: uncompatibilized PS/PA6, (PPE/PS)/PA6 and PPE/PA6 blends
    Tol, RT
    Mathot, VBF
    Groeninckx, G
    [J]. POLYMER, 2005, 46 (02) : 369 - 382
  • [48] Fabrication of PA6/MoS2 nanocomposites via melt blending of PA6 with PA6/PEG modified-MoS2 masterbatch
    Zhang, He-Xin
    Park, Joon-Young
    Lee, Dong-Eun
    Yoon, Keun-Byoung
    [J]. POLYMER BULLETIN, 2022, 79 (12) : 10639 - 10652
  • [49] Determination of a limiting dispersed phase concentration for coalescence in PA6/HDPE blends under extensional flow
    González-Nuñez, R
    Arellano, M
    Moscoso, FJ
    González-Romero, VM
    Favis, BD
    [J]. POLYMER, 2001, 42 (12) : 5485 - 5489
  • [50] Nonisothermal crystallization kinetics of PA6 and PA6/SEBS-g-MA blends
    S. N. Hemlata
    [J]. Journal of Polymer Research, 2012, 19