Creep-constitutive behavior of Sn-3.8Ag-0.7Cu solder using an internal stress approach

被引:0
|
作者
Martin A. Rist
W. J. Plumbridge
S. Cooper
机构
[1] The Open University,Department of Materials Engineering
来源
关键词
Creep; Pb-free solder; constitutive equations;
D O I
暂无
中图分类号
学科分类号
摘要
The experimental tensile creep deformation of bulk Sn-3.8Ag-0.7Cu solder at temperatures between 263 K and 398 K, covering lifetimes up to 3,500 h, has been rationalized using constitutive equations that incorporate structure-related internal state variables. Primary creep is accounted for using an evolving internal back stress, due to the interaction between the soft matrix phase and a more creep-resistant particle phase. Steady-state creep is incorporated using a conventional power law, modified to include the steady-state value of internal stress. It is demonstrated that the observed behavior is well-fitted using creep constants for pure tin in the modified creep power law. A preliminary analysis of damage-induced tertiary creep is also presented.
引用
收藏
页码:1050 / 1058
页数:8
相关论文
共 50 条
  • [21] Aging induced structural and electrochemical corrosion behaviour of Sn-1.0Ag-0.5Cu and Sn-3.8Ag-0.7Cu solder alloys
    Kaushik, Raj K.
    Batra, Uma
    Sharma, J. D.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 745 : 446 - 454
  • [22] Microstructural effects on low cycle fatigue of Sn-3.8Ag-0.7Cu Pb-free Solder
    Zeng, Qiu Lian
    Wang, Zhong Guang
    Shang, J. K.
    MECHANICAL BEHAVIOR OF MATERIALS X, PTS 1AND 2, 2007, 345-346 : 239 - +
  • [24] Solidification condition effects on microstructures and creep resistance of Sn-3.8Ag-0.7Cu lead-free
    Liang, J.
    Dariavach, N.
    Shangguan, D.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (07): : 1530 - 1538
  • [25] Cyclic softening of the Sn-3.8Ag-0.7Cu lead-free solder alloy with equiaxed grain structure
    Qiu-Lian Zeng
    Zhong-Guang Wang
    Ai-Ping Xian
    J. K. Shang
    Journal of Electronic Materials, 2005, 34 : 62 - 67
  • [26] Effects of Co nanoparticle addition to Sn-3.8Ag-0.7Cu solder on interfacial structure after reflow and ageing
    Haseeb, A. S. M. A.
    Leng, Tay See
    INTERMETALLICS, 2011, 19 (05) : 707 - 712
  • [27] Constitutive behavior of Sn3.8Ag0.7Cu and Sn1.0Ag0.5Cu alloys at creep and low strain rate regimes
    Bhate, D.
    Chan, D.
    Subbarayan, G.
    Chiu, T. C.
    Gupta, V.
    Edwards, D.
    PROCEEDINGS OF THE ASME INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION 2007, VOL 5: ELECTRONICS AND PHOTONICS, 2008, : 183 - 196
  • [28] Reliability of fine pitch Sn-3.8Ag-0.7Cu flip chip solder joints with different connection pads
    Li, Dezhi
    Liu, Changqing
    Conway, Paul P.
    2006 CONFERENCE ON HIGH DENSITY MICROSYSTEM DESIGN AND PACKAGING AND COMPONENT FAILURE ANALYSIS (HDP '06), PROCEEDINGS, 2006, : 159 - +
  • [29] Constitutive behavior of Sn3.8Ag0.7Cu and Sn1.0Ag0.5Cu alloys at creep and low strain rate regimes
    Bhate, Dhruv
    Chan, Dennis
    Subbarayan, Ganesh
    Chiu, Tz Cheng
    Gupta, Vikas
    Edwards, Darvin R.
    IEEE TRANSACTIONS ON COMPONENTS AND PACKAGING TECHNOLOGIES, 2008, 31 (03): : 622 - 633
  • [30] Characterization of IMC layer and its effect on thermomechanical fatigue life of Sn-3.8Ag-0.7Cu solder joints
    Che, F. X.
    Pang, John H. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 541 : 6 - 13