Effect of Bonding Temperature on Interfacial Reaction and Mechanical Properties of Diffusion-Bonded Joint Between Ti-6Al-4V and 304 Stainless Steel Using Nickel as an Intermediate Material

被引:2
|
作者
Gopinath Thirunavukarasu
Sukumar Kundu
Brajendra Mishra
Subrata Chatterjee
机构
[1] Bengal Engineering and Science University,Department of Metallurgy and Materials Engineering
[2] Shibpur,Department of Metallurgical and Materials Engineering
[3] Colorado School of Mines,undefined
关键词
Reaction Layer; Bonding Temperature; Diffusion Bonding; Ni3Ti; Bonding Time;
D O I
暂无
中图分类号
学科分类号
摘要
An investigation was carried out on the solid-state diffusion bonding between Ti-6Al-4V (TiA) and 304 stainless steel (SS) using pure nickel (Ni) of 200-μm thickness as an intermediate material prepared in vacuum in the temperature range from 973 K to 1073 K (700 °C to 800 °C) in steps of 298 K (25 °C) using uniaxial compressive pressure of 3 MPa and 60 minutes as bonding time. Scanning electron microscopy images, in backscattered electron mode, had revealed existence of layerwise Ti-Ni-based intermetallics such as either Ni3Ti or both Ni3Ti and NiTi at titanium alloy-nickel (TiA/Ni) interface, whereas nickel-stainless steel (Ni/SS) diffusion zone was free from intermetallic phases for all joints processed. Chemical composition of the reaction layers was determined in atomic percentage by energy dispersive spectroscopy and confirmed by X-ray diffraction study. Room-temperature properties of the bonded joints were characterized using microhardness evaluation and tensile testing. The maximum hardness value of ~800 HV was observed at TiA/Ni interface for the bond processed at 1073 K (800 °C). The hardness value at Ni/SS interface for all the bonds was found to be ~330 HV. Maximum tensile strength of ~206 MPa along with ~2.9 pct ductility was obtained for the joint processed at 1023 K (750 °C). It was observed from the activation study that the diffusion rate at TiA/Ni interface is lesser than that at the Ni/SS interface. From microhardness profile, fractured surfaces and fracture path, it was demonstrated that failure of the joints was initiated and propagated apparently at the TiA/Ni interface near Ni3Ti intermetallic phase.
引用
收藏
页码:2067 / 2077
页数:10
相关论文
共 50 条
  • [21] Microstructure and Mechanical Properties of Ti-6Al-4V Alloy/Interstitial Free Steel Joint Diffusion Bonded with Application of Copper and Nickel Interlayers
    Raj, Manil
    Prasad, M. J. N. V.
    Narasimhan, K.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2020, 51 (12): : 6234 - 6247
  • [22] Microstructure and Mechanical Properties of Ti-6Al-4V Alloy/Interstitial Free Steel Joint Diffusion Bonded with Application of Copper and Nickel Interlayers
    Manil Raj
    M. J. N. V. Prasad
    K. Narasimhan
    Metallurgical and Materials Transactions A, 2020, 51 : 6234 - 6247
  • [23] Influence of bonding time during diffusion bonding of Ti-6Al-4V to AISI 321 stainless steel on metallurgical and mechanical properties
    Wang, Hongliang
    Paidar, Moslem
    Kumar, N. Keerthi
    Eldin, Hany M. Seif
    Kannan, Sathish
    Abdullaev, Sherzod
    Mehrez, Sadok
    VACUUM, 2024, 222
  • [24] Characterization of a functionally graded material of Ti-6Al-4V to 304L stainless steel with an intermediate V section
    Bobbio, Lourdes D.
    Bocklund, Brandon
    Otis, Richard
    Borgonia, John Paul
    Dillon, R. Peter
    Shapiro, Andrew A.
    McEnerney, Bryan
    Liu, Zi-Kui
    Beese, Allison M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 742 : 1031 - 1036
  • [25] Interfacial microstructure and mechanical properties of diffusion-bonded titanium-stainless steel joints using a nickel interlayer
    Kundu, S.
    Chatterjee, S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 425 (1-2): : 107 - 113
  • [26] Diffusion bonding between Ti-6Al-4V alloy and microduplex stainless steel with copper interlayer
    Eroglu, M
    Khan, TI
    Orhan, N
    MATERIALS SCIENCE AND TECHNOLOGY, 2002, 18 (01) : 68 - 72
  • [27] Effect of Bonding Temperature on the Interfacial Microstructure and Mechanical Properties of W/Steel Joints Diffusion-Bonded with a CoFeNi Interlayer
    Wang, Chunyan
    Tao, Guoyun
    Liang, Shuibao
    Song, Kuijing
    Wang, Chengyong
    Wu, Yucheng
    Zhong, Zhihong
    JOM, 2024, 76 (11) : 6313 - 6324
  • [28] Interface microstructure and strength properties of Ti-6Al-4V and microduplex stainless steel diffusion bonded joints
    Kundu, S.
    Sam, S.
    Chatterjee, S.
    MATERIALS & DESIGN, 2011, 32 (05) : 2997 - 3003
  • [29] Effect of phase transformation and intermetallic compounds on the microstructure and tensile strength properties of diffusion-bonded joints between Ti-6Al-4V and AISI 304L
    Vigraman, T.
    Ravindran, D.
    Narayanasamy, R.
    MATERIALS & DESIGN, 2012, 36 : 714 - 727
  • [30] Effect of Processing Temperature on the Texture and Shear Mechanical Properties of Diffusion Bonded Ti-6Al-4V Multilayer Laminates
    Carmen M. Cepeda-Jiménez
    Alberto Orozco-Caballero
    Aigul Sarkeeva
    Aleksey Kruglov
    Ramil Lutfullin
    Oscar A. Ruano
    Fernando Carreño
    Metallurgical and Materials Transactions A, 2013, 44 : 4743 - 4753