Semi-solid Constitutive Parameters and Failure Behavior of a Cast AA7050 Alloy

被引:0
|
作者
Tungky Subroto
Dmitry G. Eskin
Alexis Miroux
Kjerstin Ellingsen
Mohammed M’Hamdi
Laurens Katgerman
机构
[1] Materials innovation institute (M2i),Department of Materials Science and Engineering
[2] Delft University of Technology,Department of Materials Science and Engineering
[3] BCAST,undefined
[4] Brunel University London,undefined
[5] Tomsk State University,undefined
[6] Alvance Aluminium Duffel,undefined
[7] SINTEF Materials and Chemistry,undefined
[8] Norwegian University of Science and Technology,undefined
关键词
D O I
暂无
中图分类号
学科分类号
摘要
AA7050 is an aluminum alloy with superior mechanical properties; however, it is prone to hot tearing (HT) during its production via direct-chill casting. This study focuses on extracting constitutive parameters of the alloy thermomechanical behavior in semi-solid state as well as gaining insight in its failure behavior. Tensile tests were performed using an Instron 5944 at solid fractions between 0.85 (550 °C) and 1.0 (465 °C), at deformation rates of 0.2 and 2 mm/min. The results showed that there are three mechanical behavior regimes in this solid fraction range: ductile at 1.0 (T = 465 °C) ≤ fs < 0.97 (T = 473 °C), brittle at 0.97 (T = 473 °C) ≤ fs ≤ 0.9 (T = 485 °C) and then ductile again (at 0.9 (T = 485 °C) < fs ≤ 0.85 (T = 550 °C)). Fracture surface analysis revealed that the fracture mode was mostly intergranular with fracture propagating through solid bridges as well. Semi-solid constitutive parameters were obtained by making a simple thermal model and numerical tensile tests in ALSIM software package and comparing the simulation results with experimental mechanical tests. The extracted constitutive parameters and available information from the literature support the fact that AA7050 is more susceptible to HT than AA5182 and Al-2 wt pct Cu alloys. The obtained parameters can further enhance the predictive capability of computer simulations of direct-chill casting.
引用
收藏
页码:871 / 888
页数:17
相关论文
共 50 条
  • [21] Physically based constitutive analysis and microstructural evolution of AA7050 aluminum alloy during hot compression
    Wang, S.
    Luo, J. R.
    Hou, L. G.
    Zhang, J. S.
    Zhuang, L. Z.
    MATERIALS & DESIGN, 2016, 107 : 277 - 289
  • [22] Fatigue size effect due to defects in an AA7050 alloy
    Abroug, Foued
    Pessard, Etienne
    Germain, Guenael
    Morel, Franck
    12TH INTERNATIONAL FATIGUE CONGRESS (FATIGUE 2018), 2018, 165
  • [23] Microstructural characterization of interrupted aging on an AA7050 aluminum alloy
    Jacumasso, S. C.
    Oliveira, P. H. F.
    Martins, J. P.
    Carvalho, A. L. M.
    MATERIALS CHARACTERIZATION, 2019, 152 : 180 - 187
  • [24] MICROSTRUCTURAL EVOLUTION OF AA7050 Al ALLOY PROCESSED BY ECAP
    Cardoso, E. K.
    Guido, V.
    Silva, G.
    Botta Filho, W.
    Jorge Junior, A.
    MATERIA-RIO DE JANEIRO, 2010, 15 (02): : 325 - 333
  • [25] Effect of processing parameters on quench sensitivity of an AA7050 sheet
    Zhang, Xinming
    Liu, WenJun
    Liu, ShengDan
    Zhou, MingZhe
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (03): : 795 - 802
  • [26] Deformation Behavior and Constitutive Equation Coupled the Grain Size of Semi-Solid Aluminum Alloy
    Lu, Yalin
    Li, Miaoquan
    Li, Xingcheng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2010, 19 (09) : 1337 - 1343
  • [27] Deformation Behavior and Constitutive Equation Coupled the Grain Size of Semi-Solid Aluminum Alloy
    Yalin Lu
    Miaoquan Li
    Xingcheng Li
    Journal of Materials Engineering and Performance, 2010, 19 : 1337 - 1343
  • [28] DEFORMATION BEHAVIOR AND MICROSTRUCTURE EVOLUTION OF 7050 ALUMINUM ALLOY DURING SEMI-SOLID STATE COMPRESSION PROCESS
    Liu Yunzhong
    Li Zhilong
    Gu Caixin
    ACTA METALLURGICA SINICA, 2013, 49 (12) : 1597 - 1603
  • [29] A probabilistic approach to study the effect of machined surface states on HCF behavior of a AA7050 alloy
    Abroug, Foued
    Pessard, Etienne
    Germain, Guenael
    Morel, Franck
    INTERNATIONAL JOURNAL OF FATIGUE, 2018, 116 : 473 - 489
  • [30] Thixotropic behavior of semi-solid magnesium alloy
    Chen, Hsueh-I
    Chen, Jyh-Chen
    SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES, 2006, 116-117 : 648 - 651