Hot Corrosion Behavior of Ti45Al8.5Nb Alloy: Effect of Anodization and Pre-oxidation

被引:0
|
作者
Hao-Jie Yan
Jun-Jie Xia
Lian-Kui Wu
Fa-He Cao
机构
[1] Shenzhen Campus of Sun Yat-sen University,School of Materials
[2] Zhejiang University of Technology,College of Materials Science and Engineering
关键词
Hot corrosion; TiAl alloy; Anodization; Pre-oxidation; Halogen effect;
D O I
暂无
中图分类号
学科分类号
摘要
The hot corrosion behavior of Ti45Al8.5Nb alloy was studied in the salt of Na2SO4 and/or NaCl at 700 °C. To improve the hot corrosion resistance, Ti45Al8.5Nb alloy was anodized in fluorine-containing solution and pre-oxidized in air. Results showed that the combination of anodization and pre-oxidation can efficiently enhance the hot corrosion resistance of Ti45Al8.5Nb alloy contaminated with Na2SO4 or Na2SO4 + NaCl deposits. This is because anodization and pre-oxidation result in the formation of compact Al2O3 layer which can act as a diffusion barrier to prevent sulfur, chlorine, and oxygen from attacking the alloy, therefore providing good resistance against hot corrosion. When exposed to NaCl deposit, however, no obvious improvement was achieved on the hot corrosion behavior no matter the alloy was anodized or further pre-oxidized in air.
引用
收藏
页码:1531 / 1546
页数:15
相关论文
共 50 条
  • [31] Effect of V/Nb on the Oxidation Resistance of Ti-45Al-9(V, Nb, Y) Alloy
    Chen Yuyong
    Yang Fei
    Kong Fantao
    Xiao Shulong
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 (03) : 429 - 432
  • [32] Effect of enamel coating on oxidation and hot corrosion behaviors of Ti-24Al-14Nb-3V alloy
    Xiong, Yuming
    Guan, Chunhong
    Zhu, Shenglong
    Wang, Fuhui
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2006, 15 (05) : 564 - 569
  • [33] Effect of enamel coating on oxidation and hot corrosion behaviors of Ti-24Al-14Nb-3V alloy
    Yuming Xiong
    Chunhong Guan
    Shenglong Zhu
    Fuhui Wang
    Journal of Materials Engineering and Performance, 2006, 15 : 564 - 569
  • [34] Hot deformation behavior of Ti-Al-Nb-W alloy
    Yang, Guang-Yu
    Liu, Yong
    Wang, Yan
    Tang, Hui-Ping
    Jia, Wen-Peng
    He, Wei-Wei
    Fenmo Yejin Cailiao Kexue yu Gongcheng/Materials Science and Engineering of Powder Metallurgy, 2013, 18 (03): : 357 - 362
  • [35] Effect of pre-oxidation treatment on the hot corrosion behavior of pack-cemented aluminide coatings on the K438 alloy in salt mixture
    Qing Li
    Xiaohu Yuan
    Dingjun Li
    Peng Song
    Zhenhua Li
    Taihong Huang
    Lei Wen
    Yuwei Liang
    Jiansheng Lu
    Corrosion Communications, 2022, 5 (01) : 1 - 13
  • [36] Microstructure, mechanical properties, hot deformation and oxidation behavior of Ti-45Al-5.4V-3.6Nb-0.3Y alloy
    Chen, Y. Y.
    Yang, F.
    Kong, F. T.
    Xiao, S. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 498 (01) : 95 - 101
  • [37] Effect of pre-oxidation treatment on the hot corrosion behavior of pack-cemented aluminide coatings on the K438 alloy in salt mixture
    Li, Qing
    Yuan, Xiaohu
    Li, Dingjun
    Song, Peng
    Li, Zhenhua
    Huang, Taihong
    Wen, Lei
    Liang, Yuwei
    Lu, Jiansheng
    CORROSION COMMUNICATIONS, 2022, 5 : 1 - 13
  • [38] The effect of pre-oxidation on the oxidation behaviour of Ti-alloy at 300°C in an alkaline steam
    Zu, XT
    Wang, ZG
    Feng, XD
    Huo, YZ
    Lin, LB
    Huang, XQ
    Li, YL
    SURFACE & COATINGS TECHNOLOGY, 2001, 140 (02): : 161 - 165
  • [40] Protective effect of the sputtered TiAlCrAg coating on the high-temperature oxidation and hot corrosion resistance of Ti-Al-Nb alloy
    Xi, YJ
    Wang, FH
    He, LL
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2004, 20 (06) : 724 - 727